Effect of densification on crack initiation under Vickers indentation test

被引:144
作者
Kato, Yoshinari [1 ,2 ]
Yamazaki, Hiroki [1 ]
Yoshida, Satoshi [2 ]
Matsuoka, Jun [2 ]
机构
[1] Nippon Elect Glass Co Ltd, Tech Div, Shiga 5208639, Japan
[2] Univ Shiga Prefecture, Sch Engn, Shiga 5228533, Japan
关键词
Glasses G205; Oxydes O180; Crack growth C281; Fracture F200; BRITTLENESS; GLASSES; CERAMICS;
D O I
10.1016/j.jnoncrysol.2010.07.015
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Crack initiation in various commercial glass compositions was investigated by measuring "crack resistance", which is determined by a series of Vickers indentation and counting of cracks around the indentation. The crack resistance of glass does not have clear relationship with hardness, fracture toughness, nor "brittleness" which is a ratio of the hardness to the fracture toughness. However, the crack resistance has a strong relationship with densification. Glass experiencing larger densification around the indentation shows higher crack resistance. Densification is assumed to reduce residual stress around the indentation, resulting in an increase in the crack resistance. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:1768 / 1773
页数:6
相关论文
共 13 条
[1]   DIRECT OBSERVATION AND ANALYSIS OF INDENTATION CRACKING IN GLASSES AND CERAMICS [J].
COOK, RF ;
PHARR, GM .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1990, 73 (04) :787-817
[2]  
*JIS, R1607 JIS
[3]   ELASTIC-PLASTIC INDENTATION DAMAGE IN CERAMICS - THE MEDIAN-RADIAL CRACK SYSTEM [J].
LAWN, BR ;
EVANS, AG ;
MARSHALL, DB .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1980, 63 (9-10) :574-581
[4]   HARDNESS, TOUGHNESS, AND BRITTLENESS - INDENTATION ANALYSIS [J].
LAWN, BR ;
MARSHALL, DB .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1979, 62 (7-8) :347-350
[5]  
MACEKNZIE JD, 1963, J AM CERAM SOC, V46, P470
[6]   Hardness and Low-Temperature Deformation of Silica Glass [J].
Neely, J. E. ;
Mackenzie, J. D. .
JOURNAL OF MATERIALS SCIENCE, 1968, 3 (06) :603-609
[7]   BRITTLENESS OF GLASSES BY INDENTATION [J].
SEHGAL, J ;
NAKAO, Y ;
TAKAHASHI, H ;
ITO, S .
JOURNAL OF MATERIALS SCIENCE LETTERS, 1995, 14 (03) :167-169
[8]   Brittleness of glass [J].
Sehgal, J ;
Ito, S .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 1999, 253 :126-132
[9]  
Wada M., 1974, Proc. Xth I.C.G, V11, P39
[10]   ELASTIC STRESS-FIELDS CAUSED BY INDENTING BRITTLE MATERIALS [J].
YOFFE, EH .
PHILOSOPHICAL MAGAZINE A-PHYSICS OF CONDENSED MATTER STRUCTURE DEFECTS AND MECHANICAL PROPERTIES, 1982, 46 (04) :617-628