Formic acid self-poisoning on bismuth-modified stepped electrodes

被引:60
作者
Maciá, MD [1 ]
Herrero, E [1 ]
Feliu, JM [1 ]
Aldaz, A [1 ]
机构
[1] Univ Alicante, Dept Quim Fis, E-03080 Alicante, Spain
关键词
Pt stepped surfaces; formic acid; Bi adatoms; self-poisoning;
D O I
10.1016/S0022-0728(00)00389-2
中图分类号
O65 [分析化学];
学科分类号
070302 ; 081704 ;
摘要
The poison formation reaction from formic acid has been studied on five different platinum stepped surfaces modified by irreversibly adsorbed bismuth. These surfaces combine (111) symmetry terraces of different widths and monoatomic steps having (110) and (100) symmetry. Their Miller indices are: Pt(775) and Pt(553), for the (110) steps, and Pt(15,13,13), Pt(544) and Pt(755) for the (100) steps. On these surfaces, bismuth deposits preferentially on the steps, and the deposition on the terrace takes place only once the step sites have been completely covered. Bismuth-modified Pt(111) vicinal surfaces show different behavior for the poison formation reaction from formic acid depending on the step symmetry and terrace width. Surfaces with wide terraces in each zone (Pt(775) and Pt(15,13,13)) exhibit behavior that can be compared to the Pt(111) electrode, i.e, poison formation is strongly inhibited once the bismuth is adsorbed on the terrace sites. On the other hand, for Pt(553) and Pt(755) surfaces, the effect of bismuth is not dependent on the adsorption site, i.e. similar inhibition of poisoning is observed when bismuth is deposited on the step or on the terrace sites. An intermediate case is observed for Pt(544) surfaces. These differences can be rationalized taking into account the different energies and the topography of the surfaces. (C) 2001 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:498 / 509
页数:12
相关论文
共 40 条
[1]   Formic acid oxidation on ultrathin Pd films on Au(hkl) and Pt(hkl) electrodes [J].
Baldauf, M ;
Kolb, DM .
JOURNAL OF PHYSICAL CHEMISTRY, 1996, 100 (27) :11375-11381
[2]   DIPOLE-MOMENTS ASSOCIATED WITH EDGE ATOMS - COMPARATIVE-STUDY ON STEPPED PT, AU AND W SURFACES [J].
BESOCKE, K ;
KRAHLURBAN, B ;
WAGNER, H .
SURFACE SCIENCE, 1977, 68 (01) :39-46
[3]   Induced adsorption of sulfate/bisulfate anions by submonolayer amounts of copper on deliberately stepped Pt surfaces [J].
Buller, LJ ;
Herrero, E ;
Gomez, R ;
Feliu, JM ;
Abruna, HD .
JOURNAL OF THE CHEMICAL SOCIETY-FARADAY TRANSACTIONS, 1996, 92 (20) :3757-3762
[4]   EFFECT OF BI AND SN ADATOMS ON FORMIC-ACID AND METHANOL OXIDATION AT WELL DEFINED PLATINUM SURFACES [J].
CAMPBELL, SA ;
PARSONS, R .
JOURNAL OF THE CHEMICAL SOCIETY-FARADAY TRANSACTIONS, 1992, 88 (06) :833-841
[5]   OXIDATION OF FORMIC-ACID AT NOBLE-METAL ELECTRODES .1. REVIEW OF PREVIOUS WORK [J].
CAPON, A ;
PARSONS, R .
JOURNAL OF ELECTROANALYTICAL CHEMISTRY, 1973, 44 (01) :1-7
[6]   APPLICATIONS OF REAL-TIME INFRARED-SPECTROSCOPY TO ELECTROCATALYSIS AT BIMETALLIC SURFACES .1. ELECTROOXIDATION OF FORMIC-ACID AND METHANOL ON BISMUTH-MODIFIED PT(111) AND PT(100) [J].
CHANG, SC ;
HO, YH ;
WEAVER, MJ .
SURFACE SCIENCE, 1992, 265 (1-3) :81-94
[7]  
CLAVILIER J, 1989, J ELECTROANAL CHEM, V261, P113, DOI 10.1016/0022-0728(89)87130-X
[8]   AN IRREVERSIBLE STRUCTURE SENSITIVE ADSORPTION STEP IN BISMUTH UNDERPOTENTIAL DEPOSITION AT PLATINUM-ELECTRODES [J].
CLAVILIER, J ;
FELIU, JM ;
ALDAZ, A .
JOURNAL OF ELECTROANALYTICAL CHEMISTRY, 1988, 243 (02) :419-433
[9]   INSITU PROBING OF STEP AND TERRACE SITES ON PT(S)-[N(111)X(111)] ELECTRODES [J].
CLAVILIER, J ;
ELACHI, K ;
RODES, A .
CHEMICAL PHYSICS, 1990, 141 (01) :1-14
[10]   ELECTROCHEMICAL ADSORPTION BEHAVIOR OF PLATINUM STEPPED SURFACES IN SULFURIC-ACID-SOLUTIONS [J].
CLAVILIER, J ;
ARMAND, D ;
SUN, SG ;
PETIT, M .
JOURNAL OF ELECTROANALYTICAL CHEMISTRY, 1986, 205 (1-2) :267-277