Oxidation behavior of ODS Fe-Cr-Al alloys:: Aluminum depletion and lifetime

被引:35
作者
Maréchal, L
Lesage, B
Huntz, AM
Molins, R
机构
[1] Univ Paris 11, CNRS, UMR 8647, Lab Etud Mat Hors Equilibre, F-91405 Orsay, France
[2] Ecole Natl Super Mines, CNRS, UMR 7633, Ctr Mat, F-91003 Evry, France
来源
OXIDATION OF METALS | 2003年 / 60卷 / 1-2期
关键词
ODS alloys; alumina growth; aluminum diffusion; aluminum depletion; lifetime;
D O I
10.1023/A:1024604428747
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The oxidation kinetics of two ODS Fe-Cr-Al alloys, PM 2000 and MA 956, were studied in oxygen and in air under isothermal conditions from 1000 to 1300degrees C. They both form an alpha-alumina scale and have good oxidation resistance, without any mass loss. Although the aluminum content in these alloys is higher than the minimum Al content necessary to ensure the growth of a continuous alumina scale, an aluminum depletion occurred in the substrate. This depletion allows the determination of aluminum diffusion coefficients in the ODS alloy. This method is very original and interesting as no Al-stable isotope is available. Moreover, the evolution of the aluminum concentration in the substrate allows one to determine the lifetime of these alloys: indeed, when the aluminum content decreases and becomes lower than a critical value, alumina can no longer form, and less-stable oxides grow very rapidly compared to alumina.
引用
收藏
页码:1 / 28
页数:28
相关论文
共 33 条
[1]  
AKIMOVA IA, 1983, PHYS MET METALLOGR, V56, P175
[2]  
CZYRSKAFILEMONO.A, 1993, MICROSCOPY OXIDATION, V2, P288
[3]  
GRABKE HJ, 1995, EUROPEAN FEDERATION, V14, P54
[4]   Aluminum and silicon diffusion in Fe-Cr-Al alloys [J].
Heesemann, A ;
Schmidtke, E ;
Faupel, F ;
Kolb-Telieps, A ;
Klöwer, J .
SCRIPTA MATERIALIA, 1999, 40 (05) :517-522
[5]  
HUNTZ AM, 1995, J PHYS III, V5, P1729, DOI 10.1051/jp3:1995221
[6]  
LEGALL M, 1994, PHILOS MAG A, V70, P761, DOI 10.1080/01418619408242929
[7]   Aluminium depletion in FeCrAl alloys during oxidation [J].
Lesage, B ;
Maréchal, L ;
Huntz, AM ;
Molins, R .
DIFFUSIONS IN MATERIALS: DIMAT2000, PTS 1 & 2, 2001, 194-1 :1707-1712
[8]  
LESAGE B, 1993, DEFECT DIFFUS FORUM, V95, P1061
[9]   Modeling of oxidation kinetics of Y-doped Fe-Cr-Al alloys [J].
Liu, ZY ;
Gao, W ;
He, YD .
OXIDATION OF METALS, 2000, 53 (3-4) :341-350
[10]   STUDY BY EXTENDED X-RAY ABSORPTION FINE-STRUCTURE TECHNIQUE AND MICROSCOPY OF THE CHEMICAL-STATE OF YTTRIUM IN ALPHA-POLYCRYSTALLINE ALUMINA [J].
LOUDJANI, MK ;
ROY, J ;
HUNTZ, AM ;
CORTES, R .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1985, 68 (11) :559-562