Mechanical properties of single electrospun collagen type I fibers

被引:231
作者
Yang, Lanti [1 ,2 ]
Fitie, Carel F. C. [1 ,2 ]
van der Werf, Kees O. [3 ,4 ]
Bennink, Martin L. [3 ,4 ]
Dijkstra, Pieter J. [1 ,2 ]
Feijen, Jan [1 ,2 ]
机构
[1] Univ Twente, Fac Sci & Technol, NL-7500 AE Enschede, Netherlands
[2] Univ Twente, Inst Biomed Technol BMTI, NL-7500 AE Enschede, Netherlands
[3] Univ Twente, Biophys Engn, Fac Sci & Technol, NL-7500 AE Enschede, Netherlands
[4] Univ Twente, MESa, Inst Nanotechnol, NL-7500 AE Enschede, Netherlands
关键词
electrospun fibers; collagen type I; cross-linking; atomic force microscopy; bending modulus; shear modulus;
D O I
10.1016/j.biomaterials.2007.10.058
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
The mechanical properties of single electrospun collagen fibers were investigated using scanning mode bending tests performed with an AFM. Electrospun collagen fibers with diameters ranging from 100 to 600 nm were successfully produced by electrospinning of an 8 % w/v solution of acid soluble collagen in 1,1,1,3,3,3-hexafluoro-2-propanot (HFP). Circular dichroism (CD) spectroscopy showed that 45% of the triple helical structure of collagen molecules was denatured in the electrospun fibers. The electrospun fibers were water soluble and became insoluble after cross-linking with glutaraldehyde vapor for 24 h. The bending moduli and shear moduli of both non- and crosslinked single electrospun collagen fibers were determined by scanning mode bending tests after depositing the fibers on glass substrates containing micro-channels. The bending moduli of the electrospun fibers ranged from 1.3 to 7.8 GPa at ambient conditions and ranged from 0.07 to 0.26MPa when immersed in PBS buffer. As the diameter of the fibrils increased, a decrease in bending modulus was measured clearly indicating mechanical anisotropy of the fiber. Cross-linking of the electrospun fibers with glutaraldehyde vapor increased the shear modulus of the fiber from similar to 30 to similar to 50 MPa at ambient conditions. (c) 2007 Elsevier Ltd. All rights reserved.
引用
收藏
页码:955 / 962
页数:8
相关论文
共 40 条
[31]   Tensile test of a single nanofiber using an atomic force microscope tip [J].
Tan, EPS ;
Goh, CN ;
Sow, CH ;
Lim, CT .
APPLIED PHYSICS LETTERS, 2005, 86 (07) :1-3
[32]   A review on electrospinning design and nanofibre assemblies [J].
Teo, W. E. ;
Ramakrishna, S. .
NANOTECHNOLOGY, 2006, 17 (14) :R89-R106
[33]   A method for determining the spring constant of cantilevers for atomic force microscopy [J].
Torii, A ;
Sasaki, M ;
Hane, K ;
Okuma, S .
MEASUREMENT SCIENCE AND TECHNOLOGY, 1996, 7 (02) :179-184
[34]   The effects of urea and n-propanol on collagen denaturation:: using DSC, circular dicroism and viscosity [J].
Usha, R ;
Ramasami, T .
THERMOCHIMICA ACTA, 2004, 409 (02) :201-206
[35]   Aligned biodegradable nanotibrous structure: a potential scaffold for blood vessel engineering [J].
Xu, CY ;
Inai, R ;
Kotaki, M ;
Ramakrishna, S .
BIOMATERIALS, 2004, 25 (05) :877-886
[36]  
YANG L, 2007, BIOPHYS J
[37]   Micromechanical bending of single collagen fibrils using atomic force microscopy [J].
Yang, Lanti ;
van der Werf, Kees O. ;
Koopman, Bart F. J. M. ;
Subramaniam, Vinod ;
Bennink, Martin L. ;
Dijkstra, Pieter J. ;
Feijen, Jan .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART A, 2007, 82A (01) :160-168
[38]   Characterization of the surface biocompatibility of the electrospun PCL-collagen nanofibers using fibroblasts [J].
Zhang, YZ ;
Venugopal, J ;
Huang, ZM ;
Lim, CT ;
Ramakrishna, S .
BIOMACROMOLECULES, 2005, 6 (05) :2583-2589
[39]   Crosslinking of the electrospun gelatin nanofibers [J].
Zhang, YZ ;
Venugopal, J ;
Huang, ZM ;
Lim, CT ;
Ramakrishna, S .
POLYMER, 2006, 47 (08) :2911-2917
[40]   Formation of collagen-glycosaminoglycan blended nanofibrous scaffolds and their biological properties [J].
Zhong, SP ;
Teo, WE ;
Zhu, X ;
Beuerman, R ;
Ramakrishna, S ;
Yung, LYL .
BIOMACROMOLECULES, 2005, 6 (06) :2998-3004