Effect of hydrogen donors on polymer degradation

被引:22
作者
Madras, G [1 ]
McCoy, BJ [1 ]
机构
[1] Univ Calif Davis, Dept Chem Engn & Mat Sci, Davis, CA 95616 USA
关键词
polymer degradation; hydrogen donor; molecular weight distribution; thermal decomposition;
D O I
10.1016/S0920-5861(98)00061-3
中图分类号
O69 [应用化学];
学科分类号
081704 ;
摘要
The thermal decomposition of hydrocarbon macromolecules, including polymers in solution, is influenced by the presence of hydrogen donors. Depending on the particular polymer, hydrogen donors may increase, decrease, or have no effect on degradation rate. We investigated the concentration effect of the hydrogen- (H-)donor, 6-hydroxy tetralin, on degradation of polystyrene (2 g/l) dissolved in mineral oil at 275 degrees C. The time evolution of the molecular weight distribution (MWD) was determined by gel permeation chromatography of samples from the batch reactor. The data indicated that the H-donor decreases the polystyrene degradation rate. This is in contrast to the H-donor (tetralin) enhancement of degradation for poly(styrene-allyl alcohol) dissolved in a 1-butanol solution at 150 degrees C. Because the reaction mechanism for polymer degradation involves radicals, we have developed continuous-distribution mass balances for polymers and radicals in the elementary reactions by treating molecular weight as a continuous variable. Based on reactions for initiation-termination, propagation-depropagation and H-abstraction, the model describes the various H-donor effects through relative values of rate coefficients. (C) 1998 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:321 / 332
页数:12
相关论文
共 30 条
[1]   KINETICS OF DONOR-SOLVENT LIQUEFACTION OF BULGARIAN BROWN COAL [J].
ANGELOVA, G ;
KAMENSKI, D ;
DIMOVA, N .
FUEL, 1989, 68 (11) :1434-1438
[2]  
CAMERON GG, 1967, J MACROMOL SCI, V1, P327
[3]   HYDROGENATING SUPERCRITICAL COAL EXTRACTION WITH TOLUENE, TETRALIN, MOLECULAR-HYDROGEN AND THEIR MIXTURES [J].
CANEL, M ;
HEDDEN, K ;
WILHELM, A .
FUEL, 1990, 69 (04) :471-475
[4]   EFFECT OF COAL PROPERTIES, TEMPERATURE, AND MINERAL MATTER UPON A HYDROGEN-DONOR SOLVENT DURING COAL-LIQUEFACTION [J].
CHAWLA, B ;
KEOGH, R ;
DAVIS, BH .
ENERGY & FUELS, 1989, 3 (02) :236-242
[5]   WEAK LINKS IN POLYSTYRENE [J].
CHIANTORE, O ;
CAMINO, G ;
COSTA, L .
POLYMER DEGRADATION AND STABILITY, 1981, 3 (03) :209-219
[6]   EFFECT OF SOLVENTS ON THERMAL-CRACKING OF MODEL COMPOUNDS TYPICAL OF COAL [J].
CHIBA, K ;
TAGAYA, H ;
YAMAUCHI, T ;
SATO, S .
INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 1991, 30 (06) :1141-1145
[7]  
CLOUGH RL, 1996, ACS S SER
[8]   Distribution kinetics of radical mechanisms: Reversible polymer decomposition [J].
Kodera, Y ;
McCoy, BJ .
AICHE JOURNAL, 1997, 43 (12) :3205-3214
[9]   INHIBITING ABILITIES OF HYDROAROMATICS AGAINST DETERIORATION OF HYDROCARBON PRODUCTS .1. INHIBITION OF THERMAL DETERIORATION AND ITS APPLICATION TO OIL PRODUCTS [J].
KUBO, J .
FUEL PROCESSING TECHNOLOGY, 1991, 27 (03) :263-277
[10]   EFFECT OF TETRALIN ON THE DEGRADATION OF POLYMER IN SOLUTION [J].
MADRAS, G ;
SMITH, JM ;
MCCOY, BJ .
INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 1995, 34 (12) :4222-4228