Highly bioactive P2O5-Na2O-CaO-SiO2 glass-ceramics

被引:444
作者
Peitl, O
Zanotto, ED
Hench, LL
机构
[1] Univ Fed Sao Carlos, Dept Mat Engn, LaMaV, BR-13565905 Sao Carlos, SP, Brazil
[2] Univ London Imperial Coll Sci Technol & Med, Dept Mat, London SW7 2BP, England
基金
巴西圣保罗研究基金会;
关键词
D O I
10.1016/S0022-3093(01)00822-5
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Glasses having a chemical composition between 1Na(2)O-2CaO-3SiO(2) (1N2C3S) and 1.5Na(2)O-1.5CaO-3SiO(2), containing 0, 2, 4 and 6 wt% P2O5, were crystallized to several volume percent through thermal treatments in the range 550-700 degreesC. These glasses and glass-ceramics were exposed to a simulated body fluid solution (SBF-K9 which is close to human plasma) for several time periods. Fourier transform infrared spectroscopy (FTIR) was used to determine the rate of hydroxy carbonate apatite (HCA) formation. Crystallization decreased the kinetics but did not inhibit the development of a HCA layer, even in fully crystallized ceramics. The onset time for crystallization of HCA varied from 8 h for a glass containing 6% P2O5 to 35 h for a fully crystallized 1.07Na(2)O-2CaO-3SiO(2) ceramic, The HCA layer formation of these compositions in in vitro' tests is much faster than in commercial bioactive materials such as synthetic hydroxyapatite ceramic, A/W glass-ceramic, Ceravital and Bioverit, for which the onset time usually takes at least seven days. FTIR and inductive coupled plasma studies confirmed the formation of an apatite layer which indicates bioactivity in the 1N2C3S crystal phase. X-ray diffraction experiments show that the phosphorus ions are kept in solid solution in the crystal phase. An apatite-like compound only appeared when the specimens were submitted to very long additional thermal treatments. The bioactivity of commercial materials is based on the apatite crystal phase, while the high level of bioactivity of this new generation of glass-ceramics is attained due to the combination of two mechanisms acting simultaneously, a non-phosphate bioactive crystal phase (1N2C3S) and the phosphorus ions in solid solution which are easily released from the structure, promoting a faster HCA layer formation similar to 45S5 Bioglass (R). (C) 2001 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:115 / 126
页数:12
相关论文
共 24 条
[1]  
[Anonymous], [No title captured]
[2]  
CLARK AE, 1989, J NONCRYST SOLIDS, V113, P195
[3]  
FILQUEIRAS MR, 1993, J BIOMED MATER RES, V27, P1485
[4]  
GONZALEZOLIVER CJR, 1979, THESIS U SHEFFIELD U, P175
[5]  
Greenspan D. C., 1994, BIOCERAMICS, V7, P55
[6]   THE ULTRASTRUCTURE OF THE INTERFACE BETWEEN A GLASS CERAMIC AND BONE [J].
GROSS, U ;
BRANDES, J ;
STRUNZ, V ;
BAB, I ;
SELA, J .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1981, 15 (03) :291-305
[7]  
Hench L, 1992, BIOCERAMICS, V5, P67
[8]  
Hench L L, 1988, Ann N Y Acad Sci, V523, P54, DOI 10.1111/j.1749-6632.1988.tb38500.x
[9]  
Hench L. L., 1994, BIOCERAMICS, V7, P3
[10]  
Hench L.L., 1991, Bioceramics, P155, DOI [10.1016/B978-0-7506-0269-3.50025-6, DOI 10.1016/B978-0-7506-0269-3.50025-6]