Effect of annealing treatments on positive temperature coefficient of resistance properties of barium titanate ceramics and a new model for the positive temperature coefficient of resistance effect

被引:40
作者
Gallego, MM [1 ]
West, AR
机构
[1] Univ Extremadura, Fac Ciencias, Dept Quim Inorgan, E-06071 Badajoz, Spain
[2] Univ Sheffield, Dept Mat Engn, Sheffield, S Yorkshire, England
关键词
D O I
10.1063/1.1374476
中图分类号
O59 [应用物理学];
学科分类号
摘要
Alternating current impedance has shown the presence of three electrical components in a semiconducting barium titanate ceramic that has been processed to give a positive temperature coefficient of resistance (PTCR) effect. Two of the component resistances, R-1 and R-2, each present a PTCR effect and, from the temperature dependence of their capacitances, they are attributed to different regions, nonferroelectric and ferroelectric, respectively, at the surfaces of individual grains or in the region of inter-grain contacts. The influence of isothermal annealing in air at 1000, 1100, and 1200 degreesC on these PTCR effects was investigated. At the resistance maxima, R-max and T-max, two types of dependence were found for both R-1 and R-2. At short times, R-max decreased and T-max shifted to higher temperatures; at long times, the reverse occurred and R-max increased while T-max shifted to lower temperature. Capacitance values for both regions were constant at short times but decreased at long times, indicating a thickening of the regions responsible for R-1 and R-2 at long times. The room temperature resistance R-25 was constant at short times but increased dramatically at long times, leading to a decrease in the magnitude of the PTCR effect. A model to account for the observed changes is proposed. Freshly fired ceramics are oxygen deficient and semiconducting; grain surfaces are Ti rich. Oxidative annealing creates an oxidized surface layer and an electron depletion layer just inside the grain surfaces. Counter diffusion through these layers of Ba2+ and O2- ions then occurs so as to partially restore electroneutrality; consequently, the concentration of surface acceptor states, N-s, decreases initially. On prolonged annealing, further oxidation occurs: oxide ions diffuse into the grain cores, with counter diffusion of electrons to the grain surfaces where they are trapped by additional absorbed oxygens leading to an increase in N-s. An explanation is given as to how both ferroelectric and nonferroelectric regions of the ceramics exhibit a PTCR effect. The key parameter that controls the activation barrier to conduction appears to be the polarization of the lattice associated with dipolar fluctuations and ferroelectric domains rather than with the polarizability of the different regions. (C) 2001 American Institute of Physics.
引用
收藏
页码:394 / 403
页数:10
相关论文
共 21 条
[1]   GRAIN-BOUNDARY CHEMISTRY OF BARIUM-TITANATE AND STRONTIUM-TITANATE .2. ORIGIN OF ELECTRICAL BARRIERS IN POSITIVE-TEMPERATURE-COEFFICIENT THERMISTORS [J].
CHIANG, YM ;
TAKAGI, T .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1990, 73 (11) :3286-3291
[2]   GRAIN-BOUNDARY CHEMISTRY OF BARIUM-TITANATE AND STRONTIUM-TITANATE .1. HIGH-TEMPERATURE EQUILIBRIUM SPACE-CHARGE [J].
CHIANG, YM ;
TAKAGI, T .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1990, 73 (11) :3278-3285
[3]   INTERFACIAL SEGREGATION IN PEROVSKITES - I-IV - COMMENT [J].
CHIANG, YM ;
TAKAGI, T .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1992, 75 (07) :2017-2019
[4]   ELECTRONIC-TRANSPORT BEHAVIOR IN SINGLE-CRYSTALLINE BA0.03SR0.97TIO3 [J].
CHOI, GM ;
TULLER, HL ;
GOLDSCHMIDT, D .
PHYSICAL REVIEW B, 1986, 34 (10) :6972-6979
[5]  
DANIELS J, 1979, PHILIPS TECH REV, V38, P73
[6]   INTERFACIAL SEGREGATION IN PEROVSKITES - I-IV - REPLY - COMMENT [J].
DESU, SB ;
PAYNE, DA .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1992, 75 (07) :2020-2024
[8]   RESISTIVITY ANOMALY IN DOPED BARIUM TITANATE [J].
HEYWANG, W .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1964, 47 (10) :484-490
[9]   THE POSITIVE TEMPERATURE-COEFFICIENT OF RESISTIVITY IN BARIUM-TITANATE [J].
HUYBRECHTS, B ;
ISHIZAKI, K ;
TAKATA, M .
JOURNAL OF MATERIALS SCIENCE, 1995, 30 (10) :2463-2474
[10]  
JOHNSTON DE, 1992, BR CERAM P, V49, P223