Surface microstructural modification and fracture behavior of tensile deformed polypropylene with different percentage crystallinity

被引:44
作者
Dasari, A
Rohrmann, J
Misra, RDK
机构
[1] Univ Louisiana Lafayette, Dept Chem Engn, Mat Sci & Engn Grp, Lafayette, LA 70504 USA
[2] Basell Polyolefins, D-65926 Frankfurt, Germany
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2003年 / 360卷 / 1-2期
关键词
polypropylene; microstructure; crystallinity; fracture;
D O I
10.1016/S0921-5093(03)00405-2
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Microstructural evolution during tensile deformation of injection molded polypropylene (PP) at the micro- and nano-scale level was studied using atomic force and scanning electron microscopy techniques. Atomic force microscopy (AFM) enabled microstructural changes of tensile deformed PPs with different percentage crystallinity to be captured. AFM of undeformed slow-cooled (SC-PP: high crystallinity) and water-quenched (WQ-PP: low crystallinity) PPs suggested that the fibrils are relatively more closely packed in the SC-PP with higher average surface height of similar to 7.5 nm as compared to similar to 5.4 nm in the case of WQ-PP. Tensile deformed SC-PP and WQ-PP at displacement rates of similar to 125-500 mm/min (strain rates of similar to 0.04 s(-1) to 0.16 s(-1)) indicated that the fibrils/microfibrils are aligned along the tensile axis, with WQ-PP exhibiting enhanced stretching of fibrils/microfibrils/chain-folded lamellae in comparison to SC-PP. Three fracture morphologies were identified at different strain rates, and include crazing/tearing (C), brittle fracture in association with crazing/tearing (B1), and brittle fracture together with ductile pulling of ligaments (B2). The fracture morphology exhibited by both SC-PP and WQ-PP was similar, but the percent area fraction of the three identified morphologies varied. WQ-PP with lower crystallinity was characterized by a decrease in percent of crazing/tearing (C) and brittle +crazing/tearing (B1),. and increase in brittle+ductile pulling of ligaments (B2). The fracture characteristics of PPs with differences in crystallinity was consistent with AFM observations. (C) 2003 Elsevier B.V. All rights reserved.
引用
收藏
页码:237 / 248
页数:12
相关论文
共 37 条
[1]  
ALBRECHT TR, 1999, POLYM SCI, V74, P2243
[2]   Multi-objective optimization in material design and selection [J].
Ashby, MF .
ACTA MATERIALIA, 2000, 48 (01) :359-369
[3]   ELECTRON-MICROSCOPY STUDIES OF FRACTURE PROCESSES IN AMORPHOUS THERMOPLASTICS [J].
BEAHAN, P ;
BEVIS, M ;
HULL, D .
POLYMER, 1973, 14 (03) :96-102
[4]   Tapping mode and phase imaging of biaxially oriented polyester films [J].
Beake, BD ;
Leggett, GJ ;
Shipway, PH .
SURFACE AND INTERFACE ANALYSIS, 2001, 31 (01) :39-45
[5]   Scratching maps for polymers [J].
Briscoe, BJ ;
Evans, PD ;
Pelillo, E ;
Sinha, SK .
WEAR, 1996, 200 (1-2) :137-147
[6]   Scratch hardness and deformation maps for polycarbonate and polyethylene [J].
Briscoe, BJ ;
Pelillo, E ;
Sinha, SK .
POLYMER ENGINEERING AND SCIENCE, 1996, 36 (24) :2996-3005
[7]   Scratch resistance of mineral-filled polypropylene materials [J].
Chu, J ;
Xiang, C ;
Sue, HJ ;
Hollis, RD .
POLYMER ENGINEERING AND SCIENCE, 2000, 40 (04) :944-955
[8]   Microstructural evolution during tensile deformation of polypropylenes [J].
Dasari, A ;
Rohrmann, J ;
Misra, RDK .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 351 (1-2) :200-213
[9]   Micro- and nano-scale deformation processes during scratch damage in high density polyethylene [J].
Dasari, A ;
Duncan, SJ ;
Misra, RDK .
MATERIALS SCIENCE AND TECHNOLOGY, 2003, 19 (02) :239-243
[10]   Micro- and nanoscale evaluation of scratch damage in poly(propylene)s [J].
Dasari, A ;
Rohrmann, J ;
Misra, RDK .
MACROMOLECULAR MATERIALS AND ENGINEERING, 2002, 287 (12) :889-903