Preparation of double-layered perpendicular media for fine magnetic structure

被引:9
作者
Ariake, J [1 ]
Honda, N
Ouchi, K
Iwasaki, SI
机构
[1] Akita Res Inst Adv Technol, Akita 0101623, Japan
[2] Tohoku Inst Technol, Sendai, Miyagi 9828577, Japan
关键词
high-density recording; media noise; perpendicular recording; thin-film media;
D O I
10.1109/20.908449
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Two preparation methods for sputter-deposition are examined in order to obtain a low noise double-layered layered perpendicular recording medium. Very thin intermediate layers between the recording layer and the soft magnetic backlayer was found to reduce the medium noise. Nitrogen addition to the NiFe system backlayer was also effective in reducing the noise, The medium noise reduction was attributed to the reduction in grain size and a magnetic domain size of the recording layer in both cases, An MFM image corresponding to a density beyond 50 Gbit/in(2) was observed for a medium with Co-Zr-Nb intermediate layer.
引用
收藏
页码:2411 / 2413
页数:3
相关论文
共 7 条
[1]  
Ariake J, 1999, ELEC SOC S, V98, P242
[2]  
HONDA N, 2000, IEEE T MAGN, P36
[3]  
KIYA T, P 1999 IEICE GEN C, P38
[4]  
NAKAMURA Y, 1996, IEICE T C2, V79, P204
[5]  
OUCHI K, 1999, J MAGN SOC JPN, P19
[6]  
YAMAKAWA K, 1999, J MAGN SOC JPN, P29
[7]  
YANASE S, 1999, TECHNICAL REP IEICE, V98