Oxygen transport properties of Ba0.5Sr0.5Co0.8Fe0.2O3-x and Ca0.5Sr0.5Mn0.8Fe0.2O3-x obtained from permeation and conductivity relaxation experiments

被引:49
作者
Girdauskaite, E. [1 ]
Ullmann, H. [1 ]
Vashook, V. V. [1 ]
Guth, U. [1 ]
Caraman, G. B. [2 ]
Bucher, E. [2 ]
Sitte, W. [2 ]
机构
[1] Tech Univ Dresden, D-01062 Dresden, Germany
[2] Univ Min & Met Leoben, Chair Phys Chem, A-8700 Leoben, Austria
关键词
perovskite-type oxides; permeability; electrical conductivity relaxation; diffusion; surface exchange;
D O I
10.1016/j.ssi.2008.02.042
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The oxygen exchange and transport properties of the perovskite-type oxides Ba0.5Sr0.5Co0.8Fe0.2O3-x (BSCF5582) and Ca0.5Sr0.5Mn0.8Fe0.2O3-x (CSMF5582) are investigated by oxygen permeation as well as electrical conductivity relaxation experiments. The temperature dependence of the oxygen permeation flux J(O2) of BSCF5582 in the range 600 <= T/degrees C <= 950 shows a transition from a low temperature region with higher activation energy to a high temperature region with lower activation energy. Complementary, the chemical surface exchange coefficient k(chem), the chemical diffusion coefficient D-chem and their activation energies are determined from conductivity relaxation experiments in the ranges 600 <= T/degrees C <= 750 and 70 < pO(2)/Pa < 3000. (c) 2008 Elsevier B.V. All rights reserved.
引用
收藏
页码:385 / 392
页数:8
相关论文
共 27 条
[1]  
Bouwmeester H.J.M., 1997, CRC HDB SOLID STATE, P501
[2]   Dense ceramic membranes for methane conversion [J].
Bouwmeester, HJM .
CATALYSIS TODAY, 2003, 82 (1-4) :141-150
[3]   OXYGEN-TRANSPORT IN SELECTED NONSTOICHIOMETRIC PEROVSKITE-STRUCTURE OXIDES [J].
CARTER, S ;
SELCUK, A ;
CHATER, RJ ;
KAJDA, J ;
KILNER, JA ;
STEELE, BCH .
SOLID STATE IONICS, 1992, 53 :597-605
[4]   Reactor flush time correction in relaxation experiments [J].
den Otter, MW ;
Bouwmeester, HJM ;
Boukamp, BA ;
Verweij, H .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2001, 148 (02) :J1-J6
[5]   Ion transport membrane technology for oxygen separation and syngas production [J].
Dyer, PN ;
Richards, RE ;
Russek, SL ;
Taylor, DM .
SOLID STATE IONICS, 2000, 134 (1-2) :21-33
[6]   MIXED ELECTRONIC/IONIC CONDUCTIVITY OF THE SOLID-SOLUTION LA(1-X)SRXCO(1-Y)NIYO3-DELTA (X= 0.4, 0.5, 0.6 AND Y= 0.2, 0.4, 0.6) [J].
FTIKOS, C ;
CARTER, S ;
STEELE, BCH .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1993, 12 (01) :79-86
[7]   Ceramic oxides with high oxygen exchange:: The system Sr-Co-O [J].
Girdauskaite, E. ;
Ullmann, H. ;
Vashook, V. ;
Bulow, M. ;
Guth, U. .
SOLID STATE IONICS, 2006, 177 (19-25) :1831-1835
[8]   Oxygen stoichiometry, unit cell volume, and thermodynamic quantities of perovskite-type oxides [J].
Girdauskaite, Egle ;
Ullmann, Helmut ;
Al Daroukh, Mahmoud ;
Vashook, Vladimir ;
Buelow, Martin ;
Guth, Ulrich .
JOURNAL OF SOLID STATE ELECTROCHEMISTRY, 2007, 11 (04) :469-477
[9]   Crystal structure and chemical correlation [J].
Goldschmidt, VM .
BERICHTE DER DEUTSCHEN CHEMISCHEN GESELLSCHAFT, 1927, 60 :1263-1296
[10]   Determination of the oxygen ion diffusion coefficients in mixed conductors by the volumetric measurement of the reoxidation kinetics [J].
Kriegel, R ;
Pippardt, U ;
Voigt, I .
SEPARATION AND PURIFICATION TECHNOLOGY, 2001, 25 (1-3) :127-135