Poling treatment and piezoelectric properties of potassium niobate ferroelectric single crystals

被引:107
作者
Wada, S [1 ]
Seike, A [1 ]
Tsurumi, T [1 ]
机构
[1] Tokyo Inst Technol, Grad Sch Sci & Engn, Dept Met & Ceram Sci, Meguro Ku, Tokyo 1528552, Japan
来源
JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS | 2001年 / 40卷 / 9B期
关键词
engineered domain configuration; piezoelectric constant; electromechanical coupling coefficient; potassium niobate single crystal; 2-step poling method; crystallographic orientation; domain wall motion;
D O I
10.1143/JJAP.40.5690
中图分类号
O59 [应用物理学];
学科分类号
摘要
Piezoelectric properties of potassium niobate (KNbO3) single crystals were investigated as a function of crystallographic orientations, i.e., [110](c) of polar direction and [001](c) of nonpolar direction. Prior to the piezoelectric measurements, the optimum conditions for a conventional poling method were investigated, and it was found that the optimum conditions for a conventional poling method were as follows, i.e., (a) high temperature above 100 degreesC, (b) long soaking time over 1 h, (c) slow heating and cooling rates below 1 degreesC/min, and d) lower poling current below I muA. However, fully poled KNbO3 crystals were not obtained using the conventional poling method. Thus, to achieve fully poled KNbO3 single crystals, a new 2-step, poling method was proposed. This method is composed of 2 poling stages, i.e., the I st step for non- 180 degrees domain switchings at higher temperatures under a low DC bias field, and the 2nd step for 180 degrees domain switchings at lower temperatures under a high DC bias field. Using the 2-step poling method, KNbO3 crystals were successfully poled, and then, their piezoelectric properties of k(31) modes were measured using a resonance method. The [110](c) poled KNbO3 crystals exhibited electromechanical coupling factor k(31) of 29.9% and piezoelectric constant d(31) of 18.4 pC/N while the [001](c) poled KNbO3 crystals exhibited k(31) of 31.2% and d(31) of 51.7 pC/N. The piezoelectric constant d(31) along nonpolar [001](c) direction was 2.8 times higher than that along polar [110](c) direction.
引用
收藏
页码:5690 / 5697
页数:8
相关论文
共 24 条
[1]  
*EL MAT MAN ASS JA, 1993, EMAS6100
[2]   PERMISSIBLE DOMAIN WALLS IN FERROELECTRIC SPECIES [J].
FOUSEK, J .
CZECHOSLOVAK JOURNAL OF PHYSICS SECTION B, 1971, B 21 (09) :955-&
[3]   PIEZOELECTRIC TENSOR OF KNBO3 [J].
GUNTER, P .
JAPANESE JOURNAL OF APPLIED PHYSICS, 1977, 16 (09) :1727-1728
[4]  
KUMAGAI H, 1988, DENSHIDENKITSUUSHINK, V88, P43
[5]   NEW FERROELECTRIC CRYSTALS [J].
MATTHIAS, BT .
PHYSICAL REVIEW, 1949, 75 (11) :1771-1771
[6]   DIELECTRIC PROPERTIES OF SODIUM AND POTASSIUM NIOBATES [J].
MATTHIAS, BT ;
REMEIKA, JP .
PHYSICAL REVIEW, 1951, 82 (05) :727-729
[7]  
MURATA K, 1989, ASAHI GARASU KENKYU, V39, P65
[8]  
MURATA K, 1989, KOUGAKU, V18, P148
[9]  
NAKAMURA K, 2000, 17 M FERR MAT THEIR, P25
[10]   NEUTRON STUDY OF DIFFUSE SCATTERING IN CUBIC KNBO3 [J].
NUNES, AC ;
AXE, JD ;
SHIRANE, G .
FERROELECTRICS, 1971, 2 (04) :291-+