EIS comparison on corrosion performance of PVD TiN and CrN coated mild steel in 0.5 N NaCl aqueous solution

被引:322
作者
Liu, C [1 ]
Bi, Q
Matthews, A
机构
[1] Loughborough Univ Technol, Dept Mfg Engn, Loughborough LE11 3TU, Leics, England
[2] Univ Hull, Res Ctr Surface Engn, Kingston Upon Hull HU6 7RX, N Humberside, England
关键词
EIS; corrosion; TiN; CrN; PVD coatings;
D O I
10.1016/S0010-938X(00)00188-8
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
AC electrochemical measurement techniques such as electrochemical impedance spectroscopy (EIS) are finding their usefulness in evaluation of the corrosion behaviour of physical vapour deposition coated steel systems. In this work, EIS has been employed to study the corrosion performance of two commercially available hard coatings (TiN and CrN) on mild steel substrate. In order to improve corrosion resistance, a four-layer deposit of each coating material was used. EIS data were acquired at the corrosion potential for each coating material (TiN or CrN) on mild steel in 0.5 N NaCl solution. interpretation of these spectra reveals the details of the corrosion process as the coated system is immersed in the solution by correlating the coating microstructure. Finally, visual inspection as immersion time increases provides the comparison on pit initiation and progression between TiN and CrN coated systems, as supportive evidence to the EIS analysis. (C) 2001 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:1953 / 1961
页数:9
相关论文
共 20 条
[1]   A LINEAR KRONIG-KRAMERS TRANSFORM TEST FOR IMMITTANCE DATA VALIDATION [J].
BOUKAMP, BA .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1995, 142 (06) :1885-1894
[2]   EFFECT OF COMPOSITION AND THICKNESS ON CORROSION BEHAVIOR OF TIN AND ZRN THIN-FILMS [J].
BROWN, R ;
ALIAS, MN ;
FONTANA, R .
SURFACE & COATINGS TECHNOLOGY, 1993, 62 (1-3) :467-473
[3]  
Elsener B., 1989, MATER SCI FORUM, V44-45, P29, DOI [10.4028/www.scientific.net/MSF.44-45.29, DOI 10.4028/WWW.SCIENTIFIC.NET/MSF.44-45.29]
[4]  
Ernst P., 1995, THESIS SHEFFIELD HAL, P1
[5]   CEMS of nitride coatings in agressive environments [J].
Hanzel, D ;
Agudelo, AC ;
Gancedo, JR ;
Lakatos-Varsanyi, M ;
Marco, JF .
HYPERFINE INTERACTIONS, 1998, 111 (1-4) :93-100
[6]   Improvement of the corrosion resistance of PVD hard coating-substrate systems [J].
Jehn, HA .
SURFACE & COATINGS TECHNOLOGY, 2000, 125 (1-3) :212-217
[7]   CORROSION STUDIES WITH HARD COATING SUBSTRATE SYSTEMS [J].
JEHN, HA ;
BAUMGARTNER, ME .
SURFACE & COATINGS TECHNOLOGY, 1992, 54 (1-3) :108-114
[8]   Corrosion performance of ion-plated titanium and yttrium-modified TiN coatings [J].
Jin, Zhujing ;
Liu, Changqing ;
Yu, Li ;
Wu, Weitao .
Surface and Coatings Technology, 1991, 46 (03) :307-315
[9]   Cyclic voltammetry measurements of different single-, bi- and multilayer TiN and single layer CrN coatings on low-carbon-steel substrates [J].
Lakatos-Varsanyi, M ;
Hanzel, D .
CORROSION SCIENCE, 1999, 41 (08) :1585-1598
[10]  
Li R., 1995, Materials Science Forum, V192-194, P237, DOI 10.4028/www.scientific.net/MSF.192-194.237