Fracture of nanostructured Sn/C anodes during Li-insertion

被引:20
作者
Aifantis, Katerina E. [1 ,2 ]
Haycock, Meghan [3 ]
Sanders, Paul [3 ]
Hackney, Stephen A. [1 ,3 ]
机构
[1] Aristotle Univ Thessaloniki, Lab Mech & Mat, Thessaloniki 54124, Greece
[2] Michigan Technol Univ, Dept Phys, Houghton, MI 49931 USA
[3] Michigan Technol Univ, Dept Mat Sci & Engn, Houghton, MI 49931 USA
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2011年 / 529卷
基金
欧洲研究理事会;
关键词
Microstructure; Fracture; Nanocomposites; Anodes; LITHIUM-ION BATTERIES; COMPOSITE; PERFORMANCE;
D O I
10.1016/j.msea.2011.08.060
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Sn/C nanocomposites, in the form of Sn or SnO2 islands attached on carbon surfaces, provide a high initial capacity when used as anodes in rechargeable Li-ion batteries. Upon Li-insertion, however, the Sn undergoes significant volume changes which result in fracture and, hence, a fade in capacity. In the present study a detailed electron microscopy analysis was used for the first time to document the fracture that occurred throughout the Li-insertion and de-insertion process. Particularly, scanning and transmission (SEM&TEM) electron microscopy was performed on four different Sn/C nanocomposites, before and after, electrochemical cycling. Analysis of the Sn particle size distribution showed that the greatest amount of fracture occurred during the first cycle. It was concluded that both the particle volume average and the area fraction of the as prepared Sn or SnO2 islands must be kept at low values in order to minimize fracture and, therefore, retain a stable capacity. A simple empirical expression was, hence, presented to relate the capacity with the initial microstructure. (C) 2011 Elsevier B.V. All rights reserved.
引用
收藏
页码:55 / 61
页数:7
相关论文
共 17 条
[1]  
Adpakpang K., UNPUB
[2]   Design criteria for nanostructured Li-ion batteries [J].
Aifantis, K. E. ;
Hackney, S. A. ;
Dempsey, J. P. .
JOURNAL OF POWER SOURCES, 2007, 165 (02) :874-879
[3]   Mechanical stability for nanostructured Sn- and Si-based anodes [J].
Aifantis, K. E. ;
Hackney, S. A. .
JOURNAL OF POWER SOURCES, 2011, 196 (04) :2122-2127
[4]   SnO2/C nanocomposites as anodes in secondary Li-ion batteries [J].
Aifantis, K. E. ;
Brutti, S. ;
Hackney, S. A. ;
Sarakonsri, T. ;
Scrosati, B. .
ELECTROCHIMICA ACTA, 2010, 55 (18) :5071-5076
[5]  
Aifantis K.E., J POWER SOU IN PRESS
[6]   Stable crack growth in nanostructured Li-batteries [J].
Aifantis, KE ;
Dempsey, JP .
JOURNAL OF POWER SOURCES, 2005, 143 (1-2) :203-211
[7]   Electrochemical lithiation of new graphite-nanosized tin particle materials obtained by SnCl2 reduction in organic medium [J].
Balan, L ;
Schneider, R ;
Ghanbaja, J ;
Willmann, P ;
Billaud, D .
ELECTROCHIMICA ACTA, 2006, 51 (17) :3385-3390
[8]   Colossal reversible volume changes in lithium alloys [J].
Beaulieu, LY ;
Eberman, KW ;
Turner, RL ;
Krause, LJ ;
Dahn, JR .
ELECTROCHEMICAL AND SOLID STATE LETTERS, 2001, 4 (09) :A137-A140
[9]   Tin nanoparticles formed in the presence of cellulose fibers exhibit excellent electrochemical performance as anode materials in lithium-ion batteries [J].
Caballero, A ;
Morales, J ;
Sánchez, L .
ELECTROCHEMICAL AND SOLID STATE LETTERS, 2005, 8 (09) :A464-A466
[10]   Nanostructured Sn-C composite as an advanced anode material in high-performance lithium-ion batteries [J].
Derrien, Gaelle ;
Hassoun, Jusef ;
Panero, Stefania ;
Scrosati, Bruno .
ADVANCED MATERIALS, 2007, 19 (17) :2336-+