Long-term operational lifetime and degradation analysis of P3HT: PCBM photovoltaic cells

被引:142
作者
Voroshazi, Eszter [1 ,2 ]
Verreet, Bregt [1 ,2 ]
Aernouts, Tom [1 ]
Heremans, Paul [1 ,2 ]
机构
[1] IMEC, Organ Photovolta, B-3001 Louvain, Belgium
[2] Katholieke Univ Leuven, ESAT MICAS, B-3001 Louvain, Belgium
关键词
Organic photovoltaics; P3HT:PCBM; Degradation; Interfaces; C(60); MoO(3); POLYMER SOLAR-CELLS; ORGANIC PHOTOVOLTAICS; PERFORMANCE; MECHANISMS; MORPHOLOGY; DEVICES;
D O I
10.1016/j.solmat.2010.09.007
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
We study the degradation of photovoltaic cells with poly(3-hexyl thiophene) (P3HT) and (6,6)-phenyl C(61)-butyric acid methyl ester (PCBM) blends under long-term continuous illumination as well as in shelf-life conditions, both in inert N(2) atmosphere. Degradation of the illuminated solar cells mainly occurs by a rapid decrease of the fill factor (FF) after 300 h, while short-circuit current and open-circuit voltage follow a linear decay after the initial burn-in. The sudden drop of the FF is correlated with an increase of the series resistance and proves irreversible upon annealing. Electrical measurements indicate that it stems from reduced charge extraction due to the photodegradation of the organic-electrode interfaces. Furthermore, as the external quantum efficiency (EQE) spectrum is evenly lowered over the entire wavelength range, we could exclude major changes in the blend morphology or significant changes to optical properties of the active layer. Introducing a thin C(60) layer leads to complete suppression of the FF decay over 1000 h, further proving that interface degradation dominates. Interestingly, similar improved lifetime over 1000 h was achieved by separate substitution of MoO(3) for PEDOT:PSS. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:1303 / 1307
页数:5
相关论文
共 35 条
[1]   Effect of interchain interactions on the absorption and emission of poly(3-hexylthiophene) -: art. no. 064203 [J].
Brown, PJ ;
Thomas, DS ;
Köhler, A ;
Wilson, JS ;
Kim, JS ;
Ramsdale, CM ;
Sirringhaus, H ;
Friend, RH .
PHYSICAL REVIEW B, 2003, 67 (06)
[2]   Interface investigation and engineering - achieving high performance polymer photovoltaic devices [J].
Chen, Li-Min ;
Xu, Zheng ;
Hong, Ziruo ;
Yang, Yang .
JOURNAL OF MATERIALS CHEMISTRY, 2010, 20 (13) :2575-2598
[3]   Organic tandem solar cells with complementary absorbing layers and a high open-circuit voltage [J].
Cheyns, D. ;
Rand, B. P. ;
Heremans, P. .
APPLIED PHYSICS LETTERS, 2010, 97 (03)
[4]   Accelerated lifetime measurements of P3HT:PCBM solar cells [J].
De Bettignies, Remi ;
Leroy, Jocelyne ;
Firon, Muriel ;
Sentein, Carole .
SYNTHETIC METALS, 2006, 156 (7-8) :510-513
[5]   Polymer-fullerene bulk heterojunction solar cells [J].
Deibel, Carsten ;
Dyakonov, Vladimir .
REPORTS ON PROGRESS IN PHYSICS, 2010, 73 (09)
[6]   Polymer-Fullerene Bulk-Heterojunction Solar Cells [J].
Dennler, Gilles ;
Scharber, Markus C. ;
Brabec, Christoph J. .
ADVANCED MATERIALS, 2009, 21 (13) :1323-1338
[7]   Nanoparticle-based, spray-coated silver top contacts for efficient polymer solar cells [J].
Girotto, Claudio ;
Rand, Barry P. ;
Steudel, Soeren ;
Genoe, Jan ;
Heremans, Paul .
ORGANIC ELECTRONICS, 2009, 10 (04) :735-740
[8]   Efficiency limiting factors of organic bulk heterojunction solar cells identified by electrical impedance spectroscopy [J].
Glatthaar, M. ;
Riede, M. ;
Keegan, N. ;
Sylvester-Hvid, K. ;
Zimmermann, B. ;
Niggemann, M. ;
Hinsch, A. ;
Gombert, A. .
SOLAR ENERGY MATERIALS AND SOLAR CELLS, 2007, 91 (05) :390-393
[9]   Flexible organic P3HT:PCBM bulk-heterojunction modules with more than 1 year outdoor lifetime [J].
Hauch, Jens A. ;
Schilinsky, Pavel ;
Choulis, Stelios A. ;
Childers, Richard ;
Biele, Markus ;
Brabec, Christoph J. .
SOLAR ENERGY MATERIALS AND SOLAR CELLS, 2008, 92 (07) :727-731
[10]   Degradation of organic solar cells due to air exposure [J].
Kawano, Kenji ;
Pacios, Roberto ;
Poplavskyy, Dmitry ;
Nelson, Jenny ;
Bradley, Donal D. C. ;
Durrant, James R. .
SOLAR ENERGY MATERIALS AND SOLAR CELLS, 2006, 90 (20) :3520-3530