In situ observation of hot tearing formation in succinonitrile-acetone

被引:160
作者
Farup, I
Drezet, JM
Rappaz, M
机构
[1] Ecole Polytech Fed Lausanne, Met Phys Lab, CH-1015 Lausanne, Switzerland
[2] SINTEF, Mat Technol, N-0314 Oslo, Norway
关键词
casting; defects; organic alloys; aluminium;
D O I
10.1016/S1359-6454(01)00013-1
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Hot tears have been induced during the solidification of a succinonitrile-acetone alloy by pulling the columnar dendrites in the transverse direction with a pulling stick. The opening of the mushy zone (hot tears) always occurred at grain boundaries. At low volume fraction of solid, the: opening can be compensated by leaner-solute interdendritic liquid (i.e., "healed" hot tears). At higher volume fraction of solid, hut tears directly nucleate in the interdendritic liquid or develop from pre-existing micropores induced by solidification shrinkage. Their surface (edge) is made of secondary dendrite arms, which have not yet bridged, but a few spikes have also been observed. These later spikes formed either by the necking of solid bridges established across the grain boundaries prior to pulling, or by the sudden break-up of the liquid Blm during pulling. Similar spikes have been found by SEM on the hut lear surface of an aluminium-copper alloy. (C) 2001 Published by Elsevier Science Ltd on behalf of Acta Materialia Inc.
引用
收藏
页码:1261 / 1269
页数:9
相关论文
共 21 条
[1]  
CAMPBELL J, 1991, CASTINGS
[2]   DENDRITIC SOLIDIFICATION IN BINARY-ALLOYS [J].
CHOPRA, MA ;
GLICKSMAN, ME ;
SINGH, NB .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1988, 19 (12) :3087-3096
[3]  
Clyne T., 1981, The influence of composition on solidification cracking susceptibility in binary alloy systems
[4]  
DREZET JM, 1999, FRENCH SOC METALLURG, P30
[5]   THE DEVELOPMENT OF SOLIDIFICATION MICROSTRUCTURES IN THE PRESENCE OF LATERAL CONSTRAINTS [J].
FABIETTI, LM ;
SEETHARAMAN, V ;
TRIVEDI, R .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1990, 21 (05) :1299-1310
[6]  
FABIETTI LM, 1991, NATURE PROPERTIES SE, P41
[7]   Two-phase modeling of mushy zone parameters associated with hot tearing [J].
Farup, I ;
Mo, A .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2000, 31 (05) :1461-1472
[8]   The effect of work hardening on thermally induced deformations in aluminium DC casting [J].
Farup, I ;
Mo, A .
JOURNAL OF THERMAL STRESSES, 2000, 23 (01) :71-89
[9]  
Feurer U., 1976, GIESSEREI FORSCH, V28, P75
[10]   DENDRITIC GROWTH - TEST OF THEORY [J].
GLICKSMAN, ME ;
SCHAEFER, RJ ;
AYERS, JD .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1976, 7 (11) :1747-1759