In situ X-ray diffraction study on MmNi3.85Mn0.27Al0.37Co0.38 as negative electrode in alkaline secondary batteries

被引:4
作者
Baddour-Hadjean, R
Pereira-Ramos, JP
Latroche, M
Percheron-Guégan, A
机构
[1] CNRS, LADIR, UMR 7075, F-94320 Thiais, France
[2] CNRS, LECSO, UMR 7582, F-94320 Thiais, France
[3] CNRS, LCMTR, UPR 209, F-74320 Thiais, France
关键词
intermetallic alloys; in situ XRD; NiMH batteries;
D O I
10.1016/S0013-4686(03)00416-X
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
This paper reports an in situ XRD study on the multisubstituted intermetallic compound MmNi(3.85)Mn(0.27)Al(0.37)Co(0.38) during an electrochemical charge-discharge reaction. Structural data are available through the evolution of the lattice parameters as electrochemical hydrogen absorption desorption proceeds within 0 less than or equal to x less than or equal to 4.3 H per formula unit and a satisfactory agreement is obtained with ex situ neutron diffraction data previously reported for the parent compound LaNi3.55Mn0.4Al0.3Co0.75. Preliminary results show the existence during discharge of a less expanded beta' phase compared with the fully charged P phase. (C) 2003 Elsevier Ltd. All rights reserved.