Effect of oxalic acid dihydrate on optical and electrochemical properties of sol-gel derived amorphous electrochromic WO3 films

被引:76
作者
Deepa, M [1 ]
Sharma, R [1 ]
Basu, A [1 ]
Agnihotry, SA [1 ]
机构
[1] Natl Phys Lab, New Delhi 110012, India
关键词
tungsten oxide; electrochromic; absorption coefficient; oxalic acid dihydrate; transmission modulation;
D O I
10.1016/j.electacta.2005.01.008
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Tungsten oxide (WO3) films have been prepared from an ethanolic acetylated peroxotungstic acid sol containing different amounts of an organic moiety, namely oxalic acid dihydrate (OAD) by sol-gel technique. Changing the precursor solution chemistry by varying the dopant proportion from 0 to 5 wt.% modifies the microstructure of the films, which are otherwise amorphous to X-rays. The microstructural differences as a function of OAD content are reflected in the transmission modulation in the photopic and solar regions, NIR reflectance, optical absorption coefficient, band gap, refractive index, switching kinetics, charge storage capacity and electrochemical activity of the films. The films derived from 3, 4 and 5 wt.% OAD sots exhibit superior electrochromic characteristics than the ones derived from 0, 1 and 2 wt.% OAD sots. The absorption band structure for the colored films peaks at similar to 1.4 eV and the band gap corresponding to indirect transitions between the parabolic bands narrows upon lithium ion insertion as it varies between 3.0 and 3.2 eV for virgin films and lies in the range of 2.6-3.1 eV for the electrolytically colored films. The films modulate transmission primarily by absorption; films with 3, 4 and 5 wt.% OAD are characterized by Delta T >= 70% and Delta R <= 10% at photopic wavelengths (lambda similar to 650-700 nm). As a paradigm illustrative of excellent electrochromic performance is the film obtained from a sol with 3 wt.% OAD which shows a coloration efficiency of 102 C cm(-2) (at 800 nm), fast color-bleach kinetics (t(c) similar to 192 s and t(b) similar to 28 s) and an ion storage capacity of 18.6 mC cm(-2), thereby rendering it suitable for smart window applications. (c) 2005 Elsevier Ltd. All rights reserved.
引用
收藏
页码:3545 / 3555
页数:11
相关论文
共 37 条
[31]   Influence of organic additive on the morphological, electrical and electrochromic properties of sol-gel derived WO3 coatings [J].
Sharma, N ;
Deepa, M ;
Varshney, P ;
Agnihotry, SA .
JOURNAL OF SOL-GEL SCIENCE AND TECHNOLOGY, 2000, 18 (02) :167-173
[32]   Nanocrystalline tungsten oxide thin film: Preparation, microstructure, and photochromic behavior [J].
Sun, M ;
Xu, N ;
Cao, YW ;
Yao, JN ;
Wang, EG .
JOURNAL OF MATERIALS RESEARCH, 2000, 15 (04) :927-933
[33]  
Tauc J., 1974, Amorphous and Liquid Semiconductors, P159, DOI [DOI 10.1007/978-1-4615-8705-7, 10.1007/978-1-4615-8705-7, 10.1007/978-1-4615-8705-7_4, DOI 10.1007/978-1-4615-8705-7_4]
[34]   Microstructure of laser-fired, sol-gel-derived tungsten oxide films [J].
Taylor, DJ ;
Cronin, JP ;
Allard, LF ;
Birnie, DP .
CHEMISTRY OF MATERIALS, 1996, 8 (07) :1396-1401
[35]   PEROXOTUNGSTIC ACID COATED FILMS FOR ELECTROCHROMIC DISPLAY DEVICES [J].
YAMANAKA, K ;
OAKAMOTO, H ;
KIDOU, H ;
KUDO, T .
JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 1986, 25 (09) :1420-1426
[36]   OSCILLATOR STRENGTH OF SMALL-POLARON ABSORPTION IN WOX (XLESS-THAN-OR-EQUAL-TO3) ELECTROCHROMIC THIN-FILMS [J].
YOSHIMURA, T .
JOURNAL OF APPLIED PHYSICS, 1985, 57 (03) :911-919
[37]   Mesoporous sol-gel WO3 thin films via poly(styrene-co-allyl-alcohol) copolymer templates [J].
Zayim, EO ;
Liu, P ;
Lee, SH ;
Tracy, CE ;
Turner, JA ;
Pitts, JR ;
Deb, SK .
SOLID STATE IONICS, 2003, 165 (1-4) :65-72