The decomposition behavior of as-received and oxidized TiH2 foaming-agent powder

被引:117
作者
Kennedy, AR [1 ]
Lopez, VH [1 ]
机构
[1] Univ Nottingham, Sch Mech Mat Mfg Engn & Management, Adv Mat Grp, Nottingham NG7 2RD, England
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2003年 / 357卷 / 1-2期
关键词
titanium hydride; oxidation; differential scanning calorimetry; metallic foam;
D O I
10.1016/S0921-5093(03)00211-9
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The decomposition behavior of as-received and oxidized TiH2 powder has been studied using differential scanning calorimetry and X-ray diffraction. It was found that the decomposition of TiH2 in argon occurs in two stages, firstly the reduction in the stoichiometry of the hydride to delta-TiH1.5, and secondly, with progressive heating, decomposition of the hydride to form the beta- and alpha-phases. When heating in air, at low temperatures, oxidation of the hydride to form an oxyhydride occurs and with progressive heating, the oxidation products Ti3O and TiO2 are formed in increasing quantities. Heat treatment, to reduce the stoichiometry of the hydride and form an oxide layer, does delay the evolution of gas when re-heated in argon. A balance between the delay in gas evolution and detrimental gas loss is best achieved for pre-heat treating to between 530 and 630 degreesC. (C) 2003 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:258 / 263
页数:6
相关论文
共 15 条
[1]  
Azarkh Z. M., 1970, Kristallografiya, V15, P275
[2]  
BAUMEISTER J, 1990, Patent No. 4018360
[3]  
Baumgärtner F, 2000, ADV ENG MATER, V2, P168, DOI 10.1002/(SICI)1527-2648(200004)2:4<168::AID-ADEM168>3.3.CO
[4]  
2-F
[5]   A study of aluminium foam formation - Kinetics and microstructure [J].
Duarte, I ;
Banhart, J .
ACTA MATERIALIA, 2000, 48 (09) :2349-2362
[6]   INVESTIGATION OF INTERACTIONS IN THE TIH2-O-2 SYSTEM [J].
FOKIN, VN ;
MALOV, YI ;
FOKINA, EE ;
TROITSKAYA, SL ;
SHILKIN, SP .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 1995, 20 (05) :387-389
[7]  
Gergely V, 1999, MET FOAM POROUS MET, P83
[8]   The investigation of titanium hydride oxidation process [J].
Gromov, AR ;
Kouznetsova, NN ;
Yudina, SL ;
Lunin, VV .
JOURNAL OF ALLOYS AND COMPOUNDS, 1997, 261 (1-2) :269-272
[9]   Effect of oxidation treatment and surface filming on hydrogen degassing from TiH2 [J].
Han, FS ;
Zhu, ZG ;
Gao, JC ;
Song, WH .
METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 1998, 29 (06) :1315-1319
[10]  
HELFEN L, 2001, CELLULAR METALS META, P239