摘要
A bent nickel wire was pressed against a yttria-stabilised zirconia (YSZ) surface, creating a small contact area. The Ni/YSZ interface was investigated and characteristic microstructures were found to develop during 200-300 h heat treatment at 1000 degreesC in 97% H-2/3% H2O with and without polarisation. A ridge of impurities up to 1.6 mum high was seen to develop along the Ni/YSZ/H-2 boundary. The impurity phase can be characterised as an alkali silicate phase containing Mn, Na, Ti, Mg, K, Al and Si. Most of these elements seem to be coming from impurities in the nickel. The initially flat contact area on the YSZ developed a hill and valley structure with an amplitude of 100 nm. The nickel wires showed negative imprints of the YSZ structures. (C) 2001 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:197 / 209
页数:13
相关论文
共 16 条
  • [1] Morphological changes at the interface of the nickel-yttria stabilized zirconia point electrode
    Aaberg, RJ
    Tunold, R
    Mogensen, M
    Berg, RW
    Odegard, R
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1998, 145 (07) : 2244 - 2252
  • [2] Ageing behaviour of zirconia stabilised by yttria and manganese oxide
    Appel, CC
    Bonanos, N
    Horsewell, A
    Linderoth, S
    [J]. JOURNAL OF MATERIALS SCIENCE, 2001, 36 (18) : 4493 - 4501
  • [3] Badwal S.P.S., 1991, P 2 INT S SOL OX FUE, P445
  • [5] Oxygen transport in La1-xSrxMn1-yCoyO3±δ perovskites part II.: Oxygen surface exchange
    De Souza, RA
    Kilner, JA
    [J]. SOLID STATE IONICS, 1999, 126 (1-2) : 153 - 161
  • [6] Influence of yttria concentration upon electrical properties and susceptibility to ageing of yttria-stabilised zirconias
    Gibson, IR
    Dransfield, GP
    Irvine, JTS
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1998, 18 (06) : 661 - 667
  • [7] GUINDET J, 1991, P 2 INT S SOL OX FUE, P553
  • [8] ON THE FACETING OF CERAMIC SURFACES
    HEFFELFINGER, JR
    BENCH, MW
    CARTER, CB
    [J]. SURFACE SCIENCE, 1995, 343 (1-2) : L1161 - L1166
  • [9] Holm R., 1967, Electric Contacts: Theory and Applications, DOI DOI 10.1007/978-3-662-06688-1
  • [10] JENSEN KV, 2000, MASS CHARGE TRANSPOR, P1443