Thermal degradation of wood treated with creosote

被引:15
作者
Becker, L [1 ]
Matuschek, G [1 ]
Lenoir, D [1 ]
Kettrup, A [1 ]
机构
[1] GSF Forschungszentrum Umwelt & Gesundheit, Inst Okol Chem, D-85758 Neuherberg, Germany
关键词
wood; creosote; combustion; TA-MS; pyrolysis;
D O I
10.1016/S0165-2370(00)00117-0
中图分类号
O65 [分析化学];
学科分类号
070302 ; 081704 ;
摘要
The results of investigations on the thermal behaviour of wood, wood treated with creosote, and of creosote are reported. Thermal analysis coupled with ion impact mass spectrometry as well as thermolysis in the modified Bayer-ICI-Shell combustion apparatus (BIS) were applied. The emission products from the BIS-apparatus were analysed qualitatively and quantitatively by gas chromatography coupled with a mass selective detector (GC/MSD). It is shown, that the degradation of creosote and wood treated with creosote is starting with a drying process of the wood around 75 degreesC, followed by evaporation of the creosote compounds between 180 and 400 degreesC. Wood itself is decomposed in an anaerobic process between 300 and 340 degreesC, followed by an oxidative process around 400 degreesC. The oxidative decomposition and mineralisation of creosote takes place between 400 and 600 degreesC with a maximum at 540 degreesC. (C) 2001 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:15 / 36
页数:22
相关论文
共 19 条
[1]  
BEAUMONT O, 1985, WOOD FIBER SCI, V17, P228
[2]  
BECKER L, 1997, THESIS TU MUNCHEN
[3]  
BECKER L, IN PRESS CHEMOSPHERE
[4]  
Betts W.D., 1990, P INT TAR C PAR
[5]  
Clarke ML, 1981, VET TOXICOLOGY
[7]  
CYRYS J, 1993, THESIS TUM WEIHENSTE
[8]  
HENNINGSON B, 1982, WEI C AMST
[9]   THERMAL-ANALYSIS - MASS-SPECTROMETRY AND THERMOGRAVIMETRIC ADSORPTION ON FIRE RETARDANTS [J].
KETTRUP, A ;
OHRBACH, KH ;
MATUSCHEK, G ;
JOACHIM, A .
THERMOCHIMICA ACTA, 1990, 166 :41-52
[10]   APPLICATION OF COMBINED THERMAL-ANALYSIS - MASS-SPECTROMETRY IN THE ANALYSIS OF FOSSIL-FUELS AND POLYMERS [J].
KETTRUP, A ;
OHRBACH, KH .
THERMOCHIMICA ACTA, 1985, 93 (SEP) :629-631