Low temperature sintering and piezoelectric properties in Pb(ZrxTi1-x)O3-Pb(Zn1/3Nb2/3)O3-Pb(Ni1/3Nb2/3)O3 ceramics

被引:30
作者
Ahn, CW
Song, HC
Park, SH
Nahm, S
Uchino, K
Priya, S
Lee, HG
Kang, NK
机构
[1] Korea Univ, Dept Mat Sci & Engn, Sungbuk Ku, Seoul 136701, South Korea
[2] Penn State Univ, Mat Res Lab, Int Ctr Actuators & Transducers, University Pk, PA 16802 USA
[3] Univ Texas, Dept Mat Sci & Engn, Arlington, TX 76019 USA
来源
JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS | 2005年 / 44卷 / 03期
关键词
PZT-PZNN ceramics; high-power device; low-temperature sintering;
D O I
10.1143/JJAP.44.1314
中图分类号
O59 [应用物理学];
学科分类号
摘要
High-power ceramics of the composition 0.8Pb(Zro.5Ti(0.5))O-3-0.2Pb[(Zn0.8Ni0.2)(1/3)Nb-2/3]O-3 (0.8PZT-0.2PZNN) + 0.5 wt% MnO2 have excellent piezoelectric and dielectric properties such as d(33) = 320pC/N, epsilon(T)(33)/epsilon(o) = 1227, k(p) = 0.54, and Q(m) = 1265. However, the sintering temperature of this composition is high, approximately 1200 degrees C, restricting the use of cheap base metal electrodes in the fabrication of multilayer components. In this study, we provide a solution to this problem and report a low sintering temperature high-power composition in a PZT-PZNN system. CuO and Al2O3 were selected as sintering agents. It was found that the addition of CuO can reduce the sintering temperature to 920 degrees C, but it can also significantly reduce the piezoelectric properties. The reduction of Q(m) magnitude was 81% when 0.5 wt% CuO was added. The addition of Al2O3 as a sintering agent was found to improve Q(m) magnitude but significant reductions in piezoelectric and dielectric properties were observed. The addition of excess ZnO and NiO was found to improve the density and piezoelectric properties, but it was also found to reduce Q(m) magnitude. Consequently, the optimization of the concentration of the sintering agents was carried out, and the optimized low sintering temperature high-power composition was found to be 0.875Pb(Zr0.5Ti0.5)O-3-0-125Pb[(Zn0.8Ni0.2)(1.5/3)Nb-2/3]O3 + 0.5 wt% MnO2 + 0.2 wt% CuO + 0.3 wt% Al2O3. The piezoelectric properties of the specimens of this composition sintered at 920 degrees C were found to be k(p) 0.581, Q(m) = 809, d(33) = 345 pC/N, epsilon(T)(3)/epsilon(o) = 1345, and T-c = 330 degrees C.
引用
收藏
页码:1314 / 1321
页数:8
相关论文
共 22 条
[1]   Effects of CuO and ZnO additives on sintering temperature and piezoelectric properties of 0.41Pb(Ni1/3Nb2/3)O3-0.36PbTiO3-0.23PbZrO3 ceramics [J].
Ahn, CW ;
Nahm, S ;
Ryu, JH ;
Uchino, K ;
Yoon, SJ ;
Jung, SJ ;
Song, JS .
JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS, 2004, 43 (01) :205-210
[2]   THE PROPERTIES OF LOW-TEMPERATURE FIRED PIEZOELECTRIC CERAMICS [J].
CHENG, SY ;
FU, SL ;
WEI, CC ;
KE, GM .
JOURNAL OF MATERIALS SCIENCE, 1986, 21 (02) :571-576
[3]   LOW-TEMPERATURE SINTERING OF LEAD-BASED PIEZOELECTRIC CERAMICS [J].
GUI, ZL ;
GAO, SH ;
ZHANG, XW .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1989, 72 (03) :486-491
[4]   Low-temperature sintering and properties of (Pb, Ba, Sr)(Zr, Ti, Sb)O3 piezoelectric ceramics using sintering aids [J].
Hayashi, T ;
Inoue, T ;
Akiyama, Y .
JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 1999, 38 (9B) :5549-5552
[5]  
Kaneko S, 1998, J AM CERAM SOC, V81, P1013, DOI 10.1111/j.1151-2916.1998.tb02439.x
[6]   STRUCTURAL DEPENDENCE ON SINTERING TEMPERATURE OF LEAD ZIRCONATE-TITANATE SOLID-SOLUTIONS [J].
LUCUTA, PG ;
CONSTANTINESCU, F ;
BARB, D .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1985, 68 (10) :533-537
[7]   CERAMIC COMPOSITES OF LEAD GERMANATE GLASS AND PZT CERAMICS [J].
OGAWA, T ;
SANO, A ;
SENDA, A ;
WAKINO, K .
JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 1989, 28 :91-94
[8]  
PATEL ND, 1986, AM CERAM SOC BULL, V65, P783
[9]   Multilayered unipoled piezoelectric transformers [J].
Priya, S ;
Ural, S ;
Kim, HW ;
Uchino, K ;
Ezaki, T .
JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 2004, 43 (6A) :3503-3510
[10]   Induction of combinatory characteristics by relaxor modification of Pb(Zr0.5Ti0.5)O3 [J].
Priya, S ;
Uchino, K ;
Ryu, J ;
Ahn, CW ;
Nahm, S .
APPLIED PHYSICS LETTERS, 2003, 83 (24) :5020-5022