Tungsten as target material in fusion devices

被引:166
作者
Naujoks, D
Asmussen, K
BessenrodtWeberpals, M
Deschka, S
Dux, R
Engelhardt, W
Field, AR
Fussmann, G
Fuchs, JC
GarciaRosales, C
Hirsch, S
Ignacz, P
Lieder, G
Mast, KF
Neu, R
Radtke, R
Roth, J
Wenzel, U
机构
[1] Max-Planck-Inst. F. Plasmaphysik, Euratom Association, Garching
关键词
D O I
10.1088/0029-5515/36/6/I01
中图分类号
O35 [流体力学]; O53 [等离子体物理学];
学科分类号
070204 ; 080103 ; 080704 ;
摘要
Several experiments were conducted in ASDEX Upgrade to prove the suitability of tungsten as a divertor target material under the conditions of a high density and low temperature divertor. The observed fluxes from a tungsten tile into the plasma are low, in keeping with the extremely low sputtering yields. In addition, the very favourable effect of 'prompt redeposition' (redeposition during the first gyration) could be confirmed by the experiments. Cooling of the edge region by neon injection seems permissible, i.e. neon impurity sputtering did not increase the eroded fluxes of tungsten. The transport and accumulation behaviour were investigated by means of the laser blow-off technique. No accumulation effects could be observed in ohmic discharges. In discharges with NBI heating but without ICRH, strong accumulation can occur. High heat flux tests were performed on graphite tiles coated with plasma sprayed tungsten, which withstood a thermal load of 15 MW/m(2) lasting 2 s as well as 1000 cycles of 10 MW/m(2) for 2 s without disabling damage. Owing to the encouraging results, an experiment using a tungsten divertor is planned in ASDEX Upgrade.
引用
收藏
页码:671 / 687
页数:17
相关论文
共 52 条
  • [1] 1ST WALL AND DIVERTOR PLATE SPUTTERING IN A TOKAMAK REACTOR
    ABRAMOV, VA
    IGITKHANOV, YL
    PISTUNOVICH, VI
    POZHAROV, VA
    [J]. JOURNAL OF NUCLEAR MATERIALS, 1989, 162 : 462 - 466
  • [2] ASSMUSEN K, 1995, THESIS TU MUNCHEN
  • [3] MEASUREMENTS OF CARBON AND TUNGSTEN EROSION DEPOSITION IN THE DIII-D DIVERTOR
    BASTASZ, R
    WAMPLER, WR
    CUTHBERTSON, JW
    BUCHENAUER, DA
    BROOKS, N
    JUNGE, R
    WEST, WP
    WONG, CPC
    [J]. JOURNAL OF NUCLEAR MATERIALS, 1995, 220 : 310 - 314
  • [4] Behringer K., 1988, Description of the impurity transport code `STRAHL'
  • [5] HEAT REMOVAL BY THE DIVERTOR PLATE AND LIMITER MATERIALS IN FUSION-REACTORS
    BEHRISCH, R
    VENUS, G
    [J]. JOURNAL OF NUCLEAR MATERIALS, 1993, 202 (1-2) : 1 - 9
  • [6] STRUCTURAL-MATERIALS FOR FUSION-REACTORS
    BLOOM, EE
    [J]. NUCLEAR FUSION, 1990, 30 (09) : 1879 - 1896
  • [7] BOSCH HS, 1994, I281 IPP M PLANCK I
  • [8] SURFACE EROSION ISSUES AND ANALYSIS FOR DISSIPATIVE DIVERTORS
    BROOKS, JN
    RUZIC, DN
    HAYDEN, DB
    TURKOT, RB
    [J]. JOURNAL OF NUCLEAR MATERIALS, 1995, 220 : 269 - 273
  • [9] CARDELLA A, 1994, FUSION TECHNOL, V1, P283
  • [10] PLASMA-WALL TRANSITION IN AN OBLIQUE MAGNETIC-FIELD
    CHODURA, R
    [J]. PHYSICS OF FLUIDS, 1982, 25 (09) : 1628 - 1633