Characterization of Delhi iron pillar rust by X-ray diffraction, Fourier transform infrared spectroscopy and Mossbauer spectroscopy

被引:128
作者
Balasubramaniam, R [1 ]
Kumar, AVR
机构
[1] Indian Inst Technol, Dept Mat & Met Engn, Kanpur 208016, Uttar Pradesh, India
[2] Stores Res & Dev Estab, Def Mat, Electrochem & Corros Div, Kanpur 208013, Uttar Pradesh, India
关键词
Delhi iron pillar; rust characterization; X-ray diffraction; Fourier transform infrared spectroscopy; Mossbauer spectroscopy; phosphate; amorphous iron oxyhydroxides;
D O I
10.1016/S0010-938X(00)00045-7
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Rust samples obtained from the region just below the decorative bell capital of the Delhi iron pillar (DIP) have been analyzed by X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR) and Mossbauer spectroscopy. The identification of iron hydrogen phosphate hydrate in the crystalline form by XRD was unambiguous. Very weak diffraction from the oxyhydroxides/oxides of iron was observed indicating that these phases are most likely to be present in the amorphous form in the rust. The present XRD analysis of rust obtained from an inaccessible area of the DIP has also been compared with earlier analyses of DIP rust obtained from regions accessible to the public. FTIR indicated that the constituents of the scale were gamma-, alpha-, delta -FeOOH, Fe3-xO4 and phosphate, and that the scale was hydrated. The unambiguous identification of the iron oxides/oxyhydroxides in the FTIR spectrum implied that they are present in the amorphous state, as XRD did not reveal these phases. The FTIR results have also been compared with earlier FTIR spectroscopic results of atmospheric rust formation. Mossbauer spectroscopy indicated that the rusts contained gamma -FeOOH, superparamagnetic alpha -FeOOH, delta -FeOOH and magnetite, all in the amorphous form. The Mossbauer spectrum also confirmed that iron in the crystalline iron hydrogen phosphate hydrate, whose presence was confirmed by XRD, was in the ferric state indicating that it was a stable end corrosion product. (C) 2000 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:2085 / 2101
页数:17
相关论文
共 36 条
[1]  
BAJPAI KD, 1990, INDIAN NUMISMATICS H, V1, P79
[2]   On the corrosion resistance of the Delhi iron pillar [J].
Balasubramaniam, R .
CORROSION SCIENCE, 2000, 42 (12) :2103-2129
[3]  
Balasubramaniam R, 1997, T INDIAN I METALS, V50, P23
[4]  
Balasubramaniam R., 1995, NML Technical Journal, V37, P123
[5]  
BALASUBRAMANIAM R, 2000, B METALS MUSEUM, V34, P42
[6]  
BALASUBRAMANIAM R, 1998, B METALS MUSEUM, V29, P19
[7]  
BARDGETT WE, 1963, J IRON STEEL I, V210, P3
[8]  
BOTTYAN L, CENTRAL RES I PHYSIC
[9]   MOSSBAUER SPECTROSCOPY OF STOICHIOMETRIC AND NON-STOICHIOMETRIC MAGNETITE [J].
DANIELS, JM ;
ROSENCWAIG, A .
JOURNAL OF PHYSICS AND CHEMISTRY OF SOLIDS, 1969, 30 (06) :1561-+
[10]  
DANNON J, 1968, CHEM APPL MOSSBAUER, P160