Slow transformation of mechanically dehydroxylated kaolinite to kaolinite -: an aged mechanochemically activated formamide-intercalated kaolinite study

被引:71
作者
Frost, RL
Horváth, E
Makó, É
Kristóf, J
Rédey, A
机构
[1] Univ Queensland, Sch Phys & Chem Sci, Inorgan Mat Res Program, Brisbane, Qld 4001, Australia
[2] Univ Veszprem, Dept Environm Engn & Chem Technol, H-8201 Veszprem, Hungary
[3] Univ Veszprem, Dept Silicate & Mat Engn, H-8201 Veszprem, Hungary
[4] Univ Veszprem, Dept Analyt Chem, H-8201 Veszprem, Hungary
基金
澳大利亚研究理事会;
关键词
kaolinite; mechanochemical activation; differential thermogravimetric analysis;
D O I
10.1016/S0040-6031(03)00316-2
中图分类号
O414.1 [热力学];
学科分类号
摘要
Formamide-intercalated high defect kaolinite which was mechanochemically activated for periods of time up to 6 h has been aged for up to 1 year. These modified materials were studied using a combination of X-ray diffraction, thermal analysis and DRIFT spectroscopy. Ageing of the formamide-intercalated mechanochemically activated kaolinite results in de-intercalation of the formamide and the de-intercalated kaolinite returns to its original d-spacing. Thermal analysis shows that the temperature of dehydration and dehydroxylation increase by up to 30degreesC. The temperature of the dehydroxylation of the aged samples was identical to that of the untreated kaolinite. The DRIFT spectroscopy showed that the spectrum of the aged samples approached that of the untreated kaolinite. The kaolinite showed partial de-intercalation and the 6 h sample had reformed to a mineral resembling the untreated kaolinite. The process of ageing the mechanochemically activated kaolinite enabled the reformation of the kaolinite. (C) 2003 Elsevier B.V. All rights reserved.
引用
收藏
页码:103 / 113
页数:11
相关论文
共 20 条
[1]  
[Anonymous], 1967, BERICHTE DTSCH KERAM
[2]  
ARKHIPENKO DK, 1961, IZVEST SIBIR OTDEL A, P109
[3]  
FREUND F, 1967, BER DEUT KERAM GES, V44, P392
[4]  
FREUND F, 1960, BER DTSCH KERAM GES, V37, P209
[5]   Modification of kaolinite surfaces by mechanochemical treatment [J].
Frost, RL ;
Makó, É ;
Kristóf, J ;
Horváth, E ;
Kloprogge, JT .
LANGMUIR, 2001, 17 (16) :4731-4738
[6]   Modification of the hydroxyl surface of kaolinite through mechanochemical treatment followed by intercalation with potassium acetate [J].
Frost, RL ;
Kristof, J ;
Mako, E ;
Martens, WN .
LANGMUIR, 2002, 18 (17) :6491-6498
[7]   The dehydroxylation of the kaolinite clay minerals using infrared emission spectroscopy [J].
Frost, RL ;
Vassallo, AM .
CLAYS AND CLAY MINERALS, 1996, 44 (05) :635-651
[8]  
GONZALEZ F, 1991, CLAY MINER, V26, P549
[9]  
GREGG SJ, 1954, J APPL CHEM, V4, P631
[10]  
KALININA AM, 1963, ZH NEORG KHIM+, V8, P2675