Thin TiCx films chemically vapour deposited onto cemented carbides from the TiCl4-CCl4-H-2 mixture

被引:15
作者
Konyashin, IY [1 ]
机构
[1] HARD & REFRACTORY MET RES INST,MOSCOW 113638,RUSSIA
关键词
titanium carbide; chemical vapour deposition; carbides; coatings;
D O I
10.1016/0040-6090(95)08134-8
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Results on the study of the deposition rate, structure, composition and some properties of TiCx films deposited from the TiCl4-CCl4H2 gaseous mixture when varying the CCl4/TiCl4 mole ratio are presented. The crystal lattice parameter of the films slightly increases when increasing the CCl4/TiCl4 ratio from 0.3 to 0.8. The average grain size of the TiCx films significantly decreases and their microhardness correspondingly increases when decreasing the CCl4/TiCl4 ratio from 0.5 to 0.1. The deposition rate has a maximum at the CCl4/TiCl4 ratio value of around 0.4. Due to enhanced reactivity of CCl4 compared with that of methane utilized as a carbon source in the CVD of TiCx films, it is possible to completely eliminate formation of a decarburized eta-phase underlayer in the cemented carbide substrate when depositing from the TiCl4-CCl4-H-2 mixture. The TiCx films when applied as wear-resistant coatings for cemented carbide tools allow improvement in tool lifetime comparable with that of conventional TiCx coatings chemically vapour deposited from the TiCl4-CH4-H-2 mixture.
引用
收藏
页码:37 / 44
页数:8
相关论文
共 32 条
[1]  
[Anonymous], 1976, REFRACTORY COMPOUNDS
[2]  
BAIK DS, 1984, 9TH P INT C CVD, P745
[3]   DEPOSITION OF TIXC LAYERS ON TIC HARDMETALS [J].
BARTSCH, K ;
LEONHARDT, A ;
WOLF, E ;
SCHONHERR, M ;
SEIDLER, M .
JOURNAL OF MATERIALS SCIENCE, 1987, 22 (08) :3032-3036
[4]   STUDY OF GROWTH-RATE AND FAILURE MODE OF CHEMICALLY VAPOR-DEPOSITED TIN, TICXNY AND TIC ON CEMENTED TUNGSTEN CARBIDE [J].
CHO, JS ;
NAM, SW ;
CHUN, JS .
JOURNAL OF MATERIALS SCIENCE, 1982, 17 (09) :2495-2502
[5]   RELATIONSHIP BETWEEN METAL-CUTTING PERFORMANCE AND MATERIAL PROPERTIES OF TIC-COATED CEMENTED CARBIDE CUTTING TOOLS [J].
CHO, T ;
BHAT, DG ;
WOERNER, PF .
SURFACE & COATINGS TECHNOLOGY, 1986, 29 (03) :239-246
[6]   HOW TO AVOID DECARBURIZATION OF STEEL SUBSTRATE DURING CHEMICAL VAPOR-DEPOSITION OF TITANIUM CARBIDE [J].
DERRE, A ;
TEYSSANDIER, F ;
DUCARROIR, M .
THIN SOLID FILMS, 1991, 202 (01) :125-135
[7]  
Derre A., 1987, Proceedings of the Tenth International Conference on Chemical Vapor Deposition 1987, P1190
[8]   THERMODYNAMIC ANALYSIS FOR THE CHEMICAL VAPOR-DEPOSITION OF NONSTOICHIOMETRIC TITANIUM CARBIDES [J].
GOTO, T ;
JIANG, CC ;
HIRAI, T .
JOURNAL OF THE LESS-COMMON METALS, 1990, 159 (1-2) :231-236
[9]  
HAYASHI K, 1984, J JPN SOC POWDER MET, V31, P136
[10]  
KONIG U, 1989, P 12 INT PLANS SEM M, P13