Effect of aluminum polycation solution on the morphology and VUV characteristics of BaMgAl10O17 blue phosphor prepared by spray pyrolysis

被引:13
作者
Lee, DY [1 ]
Kang, YC
Jung, KY
机构
[1] Korea Res Inst Chem Technol, Adv Mat Div, Taejon 305600, South Korea
[2] Chungnam Natl Univ, Dept Chem Engn, Taejon 305764, South Korea
关键词
D O I
10.1149/1.1615354
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Spherical BaMgAl10O17:Eu (BAM) phosphor particles with good photoluminescence characteristics under the excitation of vacuum ultraviolet light were synthesized by spray pyrolysis. Two different spray solutions were prepared to see the changes in the morphology and luminance properties of BAM particles. One was an aqueous solution; the other was a polycation solution which was obtained by chemically modifying the aqueous solution with NH4OH. The BAM particles prepared with the aqueous solution had a porous structure and utterly lost their spherical morphology after post heat-treatment. On the contrary, completely dense and spherical particles were obtained from the polycation solution and their spherical morphology was maintained even after heat-treatment. The dense and spherical BAM particles showed remarkable improvement in photoluminescence intensity compared to that of the hollow particles as well as the commercial one. According to X-ray diffraction analysis, there was no difference in the crystal structures of the two samples. So, the improved photoluminescence comes not from the difference of chemical composition or crystal structure, but from the morphological difference. (C) 2003 The Electrochemical Society.
引用
收藏
页码:H27 / H29
页数:3
相关论文
共 17 条
[1]  
BETSUI K, 1999, Patent No. 5967872
[2]  
BRINKER CJ, 1990, SOL GEL SCI PHYSICS
[3]  
HAMPDENSMITH MJ, 2001, Patent No. 6197218
[4]  
HASHIMOTO Y, 2001, SID 01, P1328
[5]  
Jüstel T, 2001, J LUMIN, V93, P179, DOI 10.1016/S0022-2313(01)00199-5
[6]  
Jüstel T, 2000, ADV MATER, V12, P527
[7]   Morphology control of BaMgAl10O17:Eu particles:: The use of colloidal solution obtained from alkoxide precursor in spray pyrolysis [J].
Kang, KC ;
Park, SB .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2000, 147 (02) :799-802
[8]   Gd2O3:Eu phosphor particles with sphericity, submicron size and non-aggregation characteristics [J].
Kang, YC ;
Park, SB ;
Lenggoro, IW ;
Okuyama, K .
JOURNAL OF PHYSICS AND CHEMISTRY OF SOLIDS, 1999, 60 (03) :379-384
[9]   Luminescence characteristics of Y2SiO5:Tb phosphor particles directly prepared by the spray pyrolysis method [J].
Kang, YC ;
Lenggoro, IW ;
Okuyama, K ;
Park, SB .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1999, 146 (03) :1227-1230
[10]   Firing technique for preparing a BaMgAl10O17:Eu2+ phosphor with controlled particle shape and size [J].
Oshio, S ;
Kitamura, K ;
Shigeta, T ;
Horii, S ;
Matsuoka, T ;
Tanaka, S ;
Kobayashi, H .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1999, 146 (01) :392-399