Control over wettability of polyethylene glycol surfaces using capillary lithography

被引:64
作者
Suh, KY [1 ]
Jon, S
机构
[1] Seoul Natl Univ, Sch Mech & Aerosp Engn, Seoul 151742, South Korea
[2] Gwangju Inst Sci & Technol, Dept Life Sci, Kwangju 500712, South Korea
关键词
D O I
10.1021/la050878+
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
We demonstrate that wettability of poly(ethylene glycol) (PEG) surfaces can be controlled using nanostructures with various geometrical features. Capillary lithography was used to fabricate PEG nanostructures using a new ultraviolet (UV) curable mold consisting of functionalized polyurethane with acrylate group (MINS101m, Minuta Tech.). Two distinct wetting states were observed depending of the height of nanostructures. At relatively lower heights (< 300 nm for 150 nm pillars with 500 nm spacing), the initial contact angle of water was less than 80 degrees and the water droplet easily invaded into the surface grooves, leading to a reduced contact angle at equilibrium (Wenzel state). At relatively higher heights (> 400 nm for 150 nm pillars with 500 nm spacing), on the other hand, the nanostructured PEG surface showed hydrophobic nature and no significant change in contact angle was observed with time (Cassie state). The presence of two wetting states was also confirmed by dynamic wetting properties and contact-angle hysteresis. The wetting transition from hydrophilic (bare PEG surface) to hydrophobic (PEG nanostructures) was described by the Cassie-Baxter equation assuming that enhanced hydrophobicity is due to the heterogeneous wetting mediated by an air pocket on the surface. The measured contact angles in the Cassie state were increased with increasing air fraction, in agreement with the theoretical prediction.
引用
收藏
页码:6836 / 6841
页数:6
相关论文
共 38 条
  • [1] ADAMSON AW, 1997, PHYSL CHEM SURFACES
  • [2] Wettability of porous surfaces.
    Cassie, ABD
    Baxter, S
    [J]. TRANSACTIONS OF THE FARADAY SOCIETY, 1944, 40 : 0546 - 0550
  • [3] Control of wettability by anion exchange on Si/SiO2 surfaces
    Chi, YS
    Lee, JK
    Lee, S
    Choi, IS
    [J]. LANGMUIR, 2004, 20 (08) : 3024 - 3027
  • [4] An ultraviolet-curable mold for sub-100-nm lithography
    Choi, SJ
    Yoo, PJ
    Baek, SJ
    Kim, TW
    Lee, HH
    [J]. JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 2004, 126 (25) : 7744 - 7745
  • [5] Switchable tackiness and wettability of a liquid crystalline polymer
    Crevoisier, GB
    Fabre, P
    Corpart, JM
    Leibler, L
    [J]. SCIENCE, 1999, 285 (5431) : 1246 - 1249
  • [6] WETTING - STATICS AND DYNAMICS
    DEGENNES, PG
    [J]. REVIEWS OF MODERN PHYSICS, 1985, 57 (03) : 827 - 863
  • [7] Stability of molded polydimethylsiloxane microstructures
    Delamarche, E
    Schmid, H
    Michel, B
    Biebuyck, H
    [J]. ADVANCED MATERIALS, 1997, 9 (09) : 741 - 746
  • [8] Transformation of a simple plastic into a superhydrophobic surface
    Erbil, HY
    Demirel, AL
    Avci, Y
    Mert, O
    [J]. SCIENCE, 2003, 299 (5611) : 1377 - 1380
  • [9] Reversible light-induced wettability of fluorine-containing azobenzene-derived Langmuir-Blodgett films
    Feng, CL
    Jin, J
    Zhang, YJ
    Song, YL
    Xie, LY
    Qu, GR
    Xu, Y
    Jiang, L
    [J]. SURFACE AND INTERFACE ANALYSIS, 2001, 32 (01) : 121 - 124
  • [10] Super-hydrophobic surfaces: From natural to artificial
    Feng, L
    Li, SH
    Li, YS
    Li, HJ
    Zhang, LJ
    Zhai, J
    Song, YL
    Liu, BQ
    Jiang, L
    Zhu, DB
    [J]. ADVANCED MATERIALS, 2002, 14 (24) : 1857 - 1860