Factors controlling the time evolution of the corrosion potential of aluminum in alkaline solutions

被引:37
作者
Adhikari, Saikat [1 ]
Hebert, Kurt R. [1 ]
机构
[1] Iowa State Univ, Dept Chem & Biol Engn, Ames, IA 50011 USA
基金
美国国家科学基金会;
关键词
aluminium; SIMS; alkaline corrosion;
D O I
10.1016/j.corsci.2008.01.001
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The mechanism of corrosion of 99.99% purity aluminum in alkaline solutions was investigated, through detailed examination of open-circuit potential transients. These transients displayed a characteristic time dependence, in which the potential first decreased over a few seconds to a minimum of -1.7 to -1.9 V vs. Ag/AgCl, and then slowly increased over a period of hours. The value of the minimum potential of electropolished foils, along with its dependence on pH and aluminate (Al(OH)(4)(-)) ion concentration, indicated that it was determined by the Nernst potential for the oxidation of surface aluminum hydride (AlH3). This finding supports the direct role of hydride in the dissolution process. The increase of anodic polarization after the minimum potential occurred in two stages, the first correlated with the buildup of surface hydride, and the second with surface enrichment of Cu and Fe impurities. (C) 2008 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1414 / 1421
页数:8
相关论文
共 36 条
[1]  
ADHIKARI S, IN PRESS J ELECTROCH
[2]   Formation of aluminum hydride during alkaline dissolution of aluminum [J].
Adhikari, Saikat ;
Lee, Jinju ;
Hebert, Kurt R. .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2008, 155 (01) :C16-C21
[3]   Effect of iron-containing intermetallic particles on the corrosion behaviour of aluminium [J].
Ambat, Rajan ;
Davenport, Alison J. ;
Scamans, Geoff M. ;
Afseth, Andreas .
CORROSION SCIENCE, 2006, 48 (11) :3455-3471
[4]   EFFECT OF TRACE-ELEMENTS ON ETCHING OF ALUMINUM ELECTROLYTIC CAPACITOR FOIL [J].
ARAI, K ;
SUZUKI, T ;
ATSUMI, T .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1985, 132 (07) :1667-1671
[5]   The behavior of copper and lead during heat-treatment and surface treatment of aluminium capacitor [J].
Ashitaka, Z ;
Thompson, GE ;
Skeldon, P ;
Wood, GC ;
Shimizu, K .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1999, 146 (04) :1380-1385
[6]   Influence of thermal and surface treatments on distributions of lead in Al-Pb foils [J].
Ashitaka, Z ;
Thompson, GE ;
Skeldon, P ;
Wood, GC ;
Habazaki, H ;
Shimizu, K .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2000, 147 (01) :132-139
[7]  
Aziz P.M., 1954, Corrosion, V10, P269
[8]   Hydrogen in aluminum [J].
Birnbaum, HK ;
Buckley, C ;
Zeides, F ;
Sirois, E ;
Rozenak, P ;
Spooner, S ;
Lin, JS .
JOURNAL OF ALLOYS AND COMPOUNDS, 1997, 253 :260-264
[9]   MICROSEGREGATION AND TENDENCY FOR PITTING CORROSION IN HIGH-PURITY ALUMINUM [J].
BOND, AP ;
BOLLING, GF ;
DOMIAN, HA ;
BILONI, H .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1966, 113 (08) :773-&
[10]   ELECTROCHEMICAL-BEHAVIOR OF ALUMINUM IN AQUEOUS CAUSTIC SOLUTIONS [J].
BROWN, OR ;
WHITLEY, JS .
ELECTROCHIMICA ACTA, 1987, 32 (04) :545-556