Molecular design of heat resistant polyimides having excellent processability and high glass transition temperature

被引:157
作者
Yokota, R
Yamamoto, S
Yano, S
Sawaguchi, T
Hasegawa, M
Yamaguchi, H
Ozawa, H
Sato, R
机构
[1] Inst Space & Astronaut Sci, Sagamihara, Kanagawa 229, Japan
[2] Nihon Univ, Fac Sci & Engn, Dept Appl Chem, Chiyoda Ku, Tokyo 101, Japan
[3] Toho Univ, Fac Sci, Dept Chem, Funabashi, Chiba 274, Japan
[4] Ube Ind Ltd, R&D, Polymer Res Lab, Chiba 290, Japan
关键词
D O I
10.1088/0954-0083/13/2/306
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The relationship between the imide structures-and morphology are discussed in order to develop heat resistant polyimides having excellent processability and toughness. Addition-type imide oligomers consisting of asymmetric 2,3,3 ' ,4 ' -biphenyltetracarboxylic dianhydride (a-BPDA) and 3,4 ' -oxydianiline (3,4 ' -ODA) and/or 4,4 ' -oxydianiline (4,4 ' -ODA) with 4-phenylethynyl phthalic anhydride (PEPA)were synthesized and characterized. The imide oligomers derived from 3,4 ' -ODA; 4,4 ' -ODA (50:50) comonomer having molecular weights of 5240 g mol(-1) (Oligo-10) and 1340 g mol(-1) (Oligo-1.5) showed good solubility in aprotic solvents such as DMAc and NMP, and were successfully cured at 370 degreesC for one hour. The thermal curing process, and thermal and rheological properties of the imide oligomers were investigated by FT-IR, differential scanning calorimetry, thermogravimetric analysis, and dynamic rheometry. It was observed that the melt flow dramatically decreased above the Tg for Oligo-1.5, resulting in a viscosity as low as 200 Poise at 300 degreesC. Whereas, a melt viscosity for Oligo-10 was 20 000 Poise at 365 degreesC. The glass transition temperatures of these cured oligomers were 341 degreesC and 308 degreesC, respectively. In addition to the excellent melt property, the cured oligomers exhibited good thermo-oxidative stability. Furthermore, the cured imide oligomer consisting of a-BPDA and 4,4 ' -ODA with PEPA (Oligo-4.5) exhibited over 13% flexural elongation and a T-g of 343 degreesC. Their T-300 carbon fibre composites were also well consolidated demonstrating excellent processability and properties. It is concluded that amorphous, aromatic imide structures without any weak linkages.
引用
收藏
页码:S61 / S72
页数:12
相关论文
共 17 条
[1]   Effect of molecular weight on processing and adhesive properties of the phenylethynyl-terminated polyimide LARC™-PETI-5 [J].
Cano, RJ ;
Jensen, BJ .
JOURNAL OF ADHESION, 1997, 60 (1-4) :113-123
[2]   Imide oligomers containing pendent and terminal phenylethynyl groups - II [J].
Connell, JW ;
Smith, JG ;
Hergenrother, PM .
HIGH PERFORMANCE POLYMERS, 1998, 10 (03) :273-283
[3]   Oligomers and polymers containing phenylethynyl groups [J].
Connell, JW ;
Smith, JG ;
Hergenrother, PM .
JOURNAL OF MACROMOLECULAR SCIENCE-REVIEWS IN MACROMOLECULAR CHEMISTRY AND PHYSICS, 2000, C40 (2-3) :207-230
[4]  
Critchley J.P., 1983, HEAT RESISTANT POLYM
[5]  
Fang XM, 1998, J POLYM SCI POL CHEM, V36, P461, DOI 10.1002/(SICI)1099-0518(199802)36:3<461::AID-POLA10>3.3.CO
[6]  
2-L
[7]  
Ghosh M. K., 1996, POLYIMIDES FUNDAMENT
[8]   Structure and properties of novel asymmetric biphenyl type polyimides. Homo- and copolymers and blends [J].
Hasegawa, M ;
Sensui, N ;
Shindo, Y ;
Yokota, R .
MACROMOLECULES, 1999, 32 (02) :387-396
[9]   CHEMISTRY AND PROPERTIES OF IMIDE OLIGOMERS END-CAPPED WITH PHENYLETHYNYLPHTHALIC ANHYDRIDES [J].
HERGENROTHER, PM ;
SMITH, JG .
POLYMER, 1994, 35 (22) :4857-4864
[10]   Processing and properties of IM7/PETI composites [J].
Hou, TH ;
Jensen, BJ ;
Hergenrother, PM .
JOURNAL OF COMPOSITE MATERIALS, 1996, 30 (01) :109-122