Effect of silver on the photocatalytic degradation of humic acid

被引:38
作者
Bansal, Ankesh [2 ]
Madhavi, S. [3 ]
Tan, Timothy Thatt Yang [1 ]
Lim, T. M. [4 ]
机构
[1] Nanyang Technol Univ, Sch Chem & Biomed Engn, Singapore 637459, Singapore
[2] Nanyang Technol Univ, Sch Civil & Environm Engn, Singapore 639798, Singapore
[3] Nanyang Technol Univ, Sch Mat Sci & Engn, Singapore 639798, Singapore
[4] Nanyang Technol Univ, Inst Environm Sci & Engn, Singapore 637723, Singapore
关键词
humic acid; TiO2; silver; photocatlysis; TEM; XPS; XRD;
D O I
10.1016/j.cattod.2007.10.078
中图分类号
O69 [应用化学];
学科分类号
081704 ;
摘要
In this study, humic acid was mineralized and degraded photocatalytically in presence of bare TiO2 and silver loaded TiO2 (0.5-5.0 at.% Ag). X-ray diffraction (XRD) and inductive coupled plasma (ICP) analysis confirm the complete photodeposition of silver over TiO2 by photodeposition method. X-ray photoemission spectroscopy (XPS) studies confirmed the presence of Ag-0 in all Ag-TiO2 samples and the absence of Ag+ ions. Silver loading over TiO2 improved the rate of mineralization and degradation of humic acid with a maximum loading of 1.0 at.% Ag. Ninety percent carbon from humic acid was mineralized to CO2 only after 60 min by using bare TiO2 as a photocatalyst. However, this conversion was possible within 40 min by using 1.0 at.% Ag-loaded TiO2. This observation verifies that coating of metals like silver over TiO2 acts as an electron sink and can improve the redox reaction by preventing electron-hole recombination reaction. The optimum 1.0 at.% Ag loading in the current work is indicative that the blocking of the TiO2 surface active sites by silver also plays an important role in the photocatalytic mineralization and degradation of humic acid. As the silver loading is increased, less number of active site are available over the surface of photocatalyst TiO2 for redox reaction. This finding was supported by the TEM analysis of the photocatalyst samples. (c) 2007 Elsevier B.V. All rights reserved.
引用
收藏
页码:250 / 254
页数:5
相关论文
共 18 条
[1]   An investigation of the photocatalytic efficiencies of TiO2 powders on the decolourisation of humic acids [J].
Bekbolet, M ;
Suphandag, AS ;
Uyguner, CS .
JOURNAL OF PHOTOCHEMISTRY AND PHOTOBIOLOGY A-CHEMISTRY, 2002, 148 (1-3) :121-128
[2]   Photocatalytic degradation and mineralization of bisphenol A by TiO2 and platinized TiO2 [J].
Chiang, K ;
Lim, TM ;
Tsen, L ;
Lee, CC .
APPLIED CATALYSIS A-GENERAL, 2004, 261 (02) :225-237
[3]   Degradation products formed during UV-irradiation of humic waters [J].
Corin, N ;
Backlund, P ;
Kulovaara, M .
CHEMOSPHERE, 1996, 33 (02) :245-255
[4]   Photocatalytic treatment of humic substances in drinking water [J].
Eggins, BR ;
Palmer, FL ;
Byrne, JA .
WATER RESEARCH, 1997, 31 (05) :1223-1226
[5]   Interactions of hypochlorite ion and humic acid:: photolytic and photocatalytic pathways [J].
Gonenç, D ;
Bekbolet, M .
WATER SCIENCE AND TECHNOLOGY, 2001, 44 (05) :205-210
[6]   Effects of acidity and inorganic ions on the photocatalytic degradation of different azo dyes [J].
Hu, C ;
Yu, JC ;
Hao, Z ;
Wong, PK .
APPLIED CATALYSIS B-ENVIRONMENTAL, 2003, 46 (01) :35-47
[7]  
HYUNG MS, 2004, PHOTOCHEM PHOTOBIO A, V163, P37
[8]   CHARGE CARRIER TRAPPING AND RECOMBINATION DYNAMICS IN SMALL SEMICONDUCTOR PARTICLES [J].
ROTHENBERGER, G ;
MOSER, J ;
GRATZEL, M ;
SERPONE, N ;
SHARMA, DK .
JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 1985, 107 (26) :8054-8059
[9]   Role of photoinduced charge carrier separation distance in heterogeneous photocatalysis: Oxidative degradation of CH3OH vapor in contact with Pt/TiO2 and cofumed TiO2-Fe2O3 [J].
Sadeghi, M ;
Liu, W ;
Zhang, TG ;
Stavropoulos, P ;
Levy, B .
JOURNAL OF PHYSICAL CHEMISTRY, 1996, 100 (50) :19466-19474
[10]  
Stevenson F. J., 1982, HUMUS CHEM GENESIS C