Sol-gel processed nanostructured CeO2-TiO2 thin films for electrochromic applications

被引:18
作者
Verma, A
Srivastava, AK
Bakhshi, AK
Kishore, R
Agnihotry, SA
机构
[1] Natl Phys Lab, Elect Mat Div, New Delhi 110012, India
[2] Univ Delhi, Dept Chem, Delhi 110007, India
关键词
electron microscopy; microstructure; sol-gel preparation; thin films;
D O I
10.1016/j.matlet.2005.06.007
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Mixed oxide films based on Cc and Ti have been deposited on transparent conducting oxide coated glass substrates using the sol-gel technique. The nanostructural characteristics of the films derived from different precursor materials (cerium chloride and ceric ammonium nitrate) have been evidenced from the transmission electron microscopic analysis. Cyclic voltammetric investigations have shown that the Li ion diffusion in the films has been influenced by the size of the CeO2 nanograins and their distribution in the amorphous TiO2 matrix. Multiple step chronoamperometric studies have revealed that the higher thickness of the films obtained using cerium chloride has resulted in the same a greater capacity to intercalate the Li ions in view of the higher number of active insertion sites for the Li ion. The latter has consequently led to improved reversibility of the electrochromic device comprising the counter electrode based on cerium chloride. The slower coloration-bleaching kinetics of the primary working electrode (WO3) in the configuration comprising the ceric ammonium nitrate based counter electrode exemplifies the advantage of using cerium chloride for depositing CeO2-TiO2 thin films for electrochromic applications. (C) 2005 Elsevier B.V. All rights reserved.
引用
收藏
页码:3423 / 3426
页数:4
相关论文
共 9 条
[1]   DIP-COATED TIO2-CEO2 FILMS AS TRANSPARENT COUNTERELECTRODE FOR TRANSMISSIVE ELECTROCHROMIC DEVICES [J].
BAUDRY, P ;
RODRIGUES, ACM ;
AEGERTER, MA ;
BULHOES, LO .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 1990, 121 (1-3) :319-322
[2]  
Brinker C.J., 1990, SOL GEL SCI
[3]  
DEROO D, 1988, Patent No. 8808809
[4]   Characterization of sputter-deposited WO3 and CeO2-x-TiO2 thin films for electrochromic applications [J].
Janke, N ;
Bieberle, A ;
Weissmann, R .
THIN SOLID FILMS, 2001, 392 (01) :134-141
[5]  
Larsson AL, 2004, MATER LETT, V58, P2517, DOI 10.1016/j,matlet.2004.03.023
[6]   ELECTROCHROMIC SMART WINDOWS [J].
MACEDO, MA ;
DALLANTONIA, LH ;
VALLA, B ;
AEGERTER, MA .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 1992, 147 :792-798
[7]   Sol-gel electrochromic WO3 coatings on glass [J].
Patra, A ;
Auddy, K ;
Ganguli, D ;
Livage, J ;
Biswas, PK .
MATERIALS LETTERS, 2004, 58 (06) :1059-1063
[8]  
TONAZZI JCL, 1990, P SOC PHOTO-OPT INS, V1328, P375, DOI 10.1117/12.22576
[9]   Optimization of CeO2-TiO2 composition for fast switching kinetics and improved Li ion storage capacity [J].
Verma, A ;
Samanta, SB ;
Bakhshi, AK ;
Agnihotry, SA .
SOLID STATE IONICS, 2004, 171 (1-2) :81-90