General and localized corrosion of magnesium alloys: A critical review

被引:378
作者
Ghali, E [1 ]
Dietzel, W
Kainer, KU
机构
[1] Univ Laval, Dept Min Met & Mat Engn, Quebec City, PQ G1K 7P4, Canada
[2] GKSS Forschungszentrum GmbH, Mat Res Inst, Ctr Magnesium Technol, Geesthacht, Germany
关键词
corrosion; magnesium; magnesium alloys;
D O I
10.1361/10599490417533
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Magnesium (Mg) alloys as well as experimental alloys are emerging as light structural materials for current, new, and innovative applications. This paper describes the influence of the alloying elements and the different casting processes on the microstructure and performance of these alloys and corrosion. It gives a comprehensible approach for the resistance of these alloys to general, localized and metallurgically influenced corrosion, which are the main challenges for,their use. Exposure to humid air with -65% relative humidity during 4 days gives 100-150 nm thickness. The film is amorphous and has an oxidation rate less than 0.01 mum/y. The pH values between 8.5 and 11.5 correspond to a relatively protective oxide or hydroxide film; however above 11.5 a passive stable layer is observed. The poor corrosion resistance of many Mg alloys can be due to the internal galvanic corrosion caused by second phases or impurities. Agitation or any other means of destroying or preventing the formation of a protective film leads to increasing corrosion kinetics. The pH changes during pitting corrosion can come from two different reduction reactions: reduction of dissolved oxygen (0) and that of hydrogen (H) ions. Filiform corrosion was observed in the uncoated AZ31, while general corrosion mainly occurred in some deposition coated alloys. Crevice corrosion can probably be initiated due to the hydrolysis reaction. Exfoliation can be considered as a type of intergranular attack, and this is observed in unalloyed Mg above a critical chloride concentration.
引用
收藏
页码:7 / 23
页数:17
相关论文
共 69 条
[1]  
Aghion E, 2003, MAGNESIUM TECHNOLOGY 2003, P177
[2]  
[Anonymous], 1999, ASM SPECIALTY HDB MA
[3]  
[Anonymous], MAGNESIUM ALLOYS THE
[4]  
[Anonymous], P 2 INT C ENV SENS C
[5]  
Bakke P, 2003, MAGNESIUM TECHNOLOGY 2003, P171
[6]   DEVELOPMENT OF CORROSION-RESISTANT MAGNESIUM ALLOYS .1. CHARACTERIZATION OF SPLAT QUENCHED MG-10AL AND MG-16AL ALLOYS [J].
BALIGA, CB ;
TSAKIROPOULOS, P .
MATERIALS SCIENCE AND TECHNOLOGY, 1993, 9 (06) :507-511
[7]  
BALOUN CH, 1987, CORROSION ASM METALS, V13, P207
[8]   The corrosion of pure magnesium in aerated and deaerated sodium sulphate solutions [J].
Baril, G ;
Pébère, N .
CORROSION SCIENCE, 2001, 43 (03) :471-484
[9]  
Beals R, 2003, MAGNESIUM TECHNOLOGY 2003, P283
[10]   INFLUENCE OF HOMOGENIZATION AND ARTIFICIAL AGING HEAT-TREATMENTS ON CORROSION BEHAVIOR OF MG-AL ALLOYS [J].
BELDJOUDI, T ;
FIAUD, C ;
ROBBIOLA, L .
CORROSION, 1993, 49 (09) :738-745