Corrosion behaviour of commercially pure titanium shot blasted with different materials and sizes of shot particles for dental implant applications

被引:226
作者
Aparicio, C
Gil, FJ
Fonseca, C
Barbosa, M
Planell, JA
机构
[1] Univ Politecn Cataluna, Dept Mat Sci & Met Engn, CREB, E-08028 Barcelona, Spain
[2] Univ Porto, Inst Engn Biomed, Lab Biomat, P-4150180 Oporto, Portugal
关键词
titanium; dental implant; shot blasting; corrosion; electrochemical impedance spectroscopy;
D O I
10.1016/S0142-9612(02)00314-9
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
It is well known that the osseointegration of the commercially pure titanium (c.p. Ti) dental implant is improved when the metal is shot blasted in order to increase its surface roughness. This roughness is colonised by bone, which improves implant fixation. However, shot blasting also changes the chemical composition of the implant surface because some shot particles remain adhered on the metal. The c.p. Ti surfaces shot blasted with different materials and sizes of shot particles were tested in order to determine their topographical features (surface roughness, real surface area and the percentage of surface covered by the adhered shot particles) and electrochemical behaviour (open circuit potential, electrochemical impedance spectroscopy and cyclic polarisation). The results demonstrate that the increased surface area of the material because of the increasing surface roughness is not the only cause for differences found in the electrochemical behaviour and corrosion resistance of the blasted c.p. Ti. Among other possible causes, those differences may be attributed to the compressive residual surface stresses induced by shot blasting. All the materials tested have an adequate corrosion and electrochemical behaviour in terms of its possible use as dental implant material. (C) 2002 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:263 / 273
页数:11
相关论文
共 61 条
  • [1] OSSEOINTEGRATED TITANIUM IMPLANTS - REQUIREMENTS FOR ENSURING A LONG-LASTING, DIRECT BONE-TO-IMPLANT ANCHORAGE IN MAN
    ALBREKTSSON, T
    BRANEMARK, PI
    HANSSON, HA
    LINDSTROM, J
    [J]. ACTA ORTHOPAEDICA SCANDINAVICA, 1981, 52 (02): : 155 - 170
  • [2] [Anonymous], 1989, EQUIVALENT CIRCUIT E
  • [3] APARICIO C, 1998, N SEA BIOM 1998 P TH, P137
  • [4] Arnell RD, 1991, Tribology: principles and design applications
  • [5] *ASTM, 1992, 1992 ANN BOOK ASTM S, P102
  • [6] *ASTM, 1992, 1992 ANN BOOK ASTM S, P231
  • [7] Electrochemical studies on the stability and corrosion resistance of titanium-based implant materials
    Aziz-Kerrzo, M
    Conroy, KG
    Fenelon, AM
    Farrell, ST
    Breslin, CB
    [J]. BIOMATERIALS, 2001, 22 (12) : 1531 - 1539
  • [8] BOHN P, 1999, SHOT PEENER, V13, P6
  • [9] Bowers K T, 1992, Int J Oral Maxillofac Implants, V7, P302
  • [10] Boyan BD, 1995, CELL MATER, V5, P323