Polyhydrazides based on 2,5-bis(4-carboxymethylene phenyl)-3,4-diphenyl thiophene

被引:22
作者
Ubale, V. P.
Patil, A. S.
Maldar, N. N. [1 ]
机构
[1] Solapur Univ, Dept Chem, Solapur 413255, India
[2] Natl Chem Lab, Div Polymer Sci & Engn, Pune 411008, Maharashtra, India
[3] DBF Dayanand Coll Arts & Sci, Solapur 413002, India
关键词
2,5-bis(4-carboxymethylene phenyl)-3,4-diphenyl thiophene; aromatic-aliphatic soluble polyhydrazides; direct polycondensation; Yamazaki's phosphorylation polycondensation; thermal properties;
D O I
10.1016/j.eurpolymj.2006.10.027
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
A series of polyhydrazides was synthesized from a novel dicarboxylic acid, 2,5-bis(4-carboxymethylene phenyl)-3, 4-diphenyl thiophene (V) and or terephthalic acid and isophthaloyl or terephthaloyl dihydrazide by Yamazaki's phosphorylation method using triphenyl phosphite as condensing agent. Polyhydrazides were characterized by IR spectroscopy solubility, viscosity, thermogravimetric analysis and X-ray diffraction studies. The polymers were obtained in quantitative yields. Polyhydrazides had viscosities in the range of 0.25-0.70 dL/g. The polymers derived from novel diacid (V) showed enhanced solubility than the polymers derived from terephthalic acid, which may be attributed to the presence to bulky pendant phenyl group and methylene spacer group in the polymer backbone. Polymers were soluble in most of the common aprotic polar solvents. Polyhydrazides showed considerable weight loss in the temperature range of 300-400 degrees C which is due to the cyclodehydration, leading to the formation of corresponding polyoxadiazoles. They showed T-max in between 500 and 600 degrees C which is essentially the decomposition of the polyoxadiazoles. X-ray diffraction studies showed that polyhydrazides were amorphous in nature. (c) 2006 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1038 / 1045
页数:8
相关论文
共 13 条
[1]  
BEAMAN RG, 1962, Patent No. 3040003
[2]   Synthesis and characterization of processable heat resistant poly (amide-imides) for high temperature applications [J].
Bhuvana, S ;
Madhumathi, M ;
Sarojadevi, M .
POLYMER BULLETIN, 2006, 57 (01) :61-72
[3]  
FISHER JW, 1954, J APPL CHEM, V4, P212
[4]   AROMATIC POLYHYDRAZIDES - NEW CLASS OF HIGHLY BONDED STIFF POLYMERS [J].
FRAZER, AH ;
WALLENBERGER, FT .
JOURNAL OF POLYMER SCIENCE PART A-GENERAL PAPERS, 1964, 2 (3PA) :1147-&
[5]   POLYIMIDES FROM DIAMINES AND DIANHYDRIDES [J].
GHATGE, ND ;
KHUNE, GD .
ANGEWANDTE MAKROMOLEKULARE CHEMIE, 1979, 79 (JUN) :93-106
[6]   DIRECT POLYESTERIFICATION BY USE OF PHOSPHORUS OXYCHLORIDE AND LICL IN PYRIDINE [J].
HIGASHI, F ;
KOBAYASHI, A ;
SHIMAZAKI, H .
JOURNAL OF POLYMER SCIENCE PART A-POLYMER CHEMISTRY, 1993, 31 (05) :1301-1305
[7]  
MOLDENHAUR O, 1944, Patent No. 2349979
[8]   Main-chain liquid crystalline poly(ester-amide)s containing lithocholic acid units [J].
Shaikh, VAE ;
Ubale, VP ;
Maldar, NN ;
Lonikar, SV ;
Rajan, CR ;
Ponrathnam, S .
JOURNAL OF APPLIED POLYMER SCIENCE, 2006, 100 (01) :73-80
[9]  
Ubale VP, 2001, J APPL POLYM SCI, V79, P566, DOI 10.1002/1097-4628(20010118)79:3<566::AID-APP200>3.0.CO
[10]  
2-J