The limiting factor for oxygen exchange at the surface of fuel cell electrolytes

被引:91
作者
de Ridder, M [1 ]
Vervoort, AGJ [1 ]
van Welzenis, RG [1 ]
Brongersma, HH [1 ]
机构
[1] Eindhoven Univ Technol, Dept Appl Phys, NL-5600 MB Eindhoven, Netherlands
关键词
surface composition; impurities; oxygen exchange; yttria stabilised zirconia (YSZ); low energy ion scattering (LEIS); YTTRIA-ZIRCONIA; STABILIZED ZIRCONIA; TETRAGONAL ZIRCONIA; Y-TZP; SEGREGATION; CONDUCTIVITY; IMPURITIES; TRANSPORT; CATHODES; KINETICS;
D O I
10.1016/S0167-2738(02)00754-3
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The outermost surface layer of the yttria stabilised zirconia (YSZ) electrolyte in the solid oxide fuel cell plays an important role in the performance of the cell. By combining O-16/O-18 exchange experiments with quantitative surface analysis by low energy ion scattering spectroscopy (LEIS), the relation between the composition of the outermost atomic layer and the oxygen kinetics at the surface of the electrolyte can be studied. The results suggest a linear relation between an increasing amount of impurity oxides present at the surface and a decreasing oxygen exchange. Ceramics invariably contain glassy impurities, which segregate to the grain boundaries during sintering. Our results, however, show that the accumulation is restricted to the outermost atomic layer and proceeds until complete coverage is obtained. This observation underlines the importance of the used surface analysis technique. The strong accumulation of the impurities at the surface is observed even in the purest YSZ materials available. A decrease of the total bulk impurity concentration by a factor of 10-100 is necessary to ensure that the YSZ surface cannot be covered completely by impurities. The amount of exchanged oxygen at the outermost surface layer reduces from 50% at a clean yttria stabilised zirconia surface to zero at a surface completely covered by impurity oxides. Although the oxygen exchange experiments pertain to a temperature of 500 degreesC it is believed that the impurity oxides also have a strong influence at higher temperatures. (C) 2003 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:255 / 262
页数:8
相关论文
共 33 条
[1]   Time dependence of the oxygen exchange O2⇆SiO2 at the SiO2-Si interface during dry thermal oxidation of silicon [J].
Åkermark, T ;
Gosset, LG ;
Ganem, JJ ;
Trimaille, I ;
Vickridge, I ;
Rigo, S .
JOURNAL OF APPLIED PHYSICS, 1999, 86 (02) :1153-1155
[2]   Solute segregation and grain-boundary impedance in high-purity stabilized zirconia [J].
Aoki, M ;
Chiang, YM ;
Kosacki, I ;
Lee, IJR ;
Tuller, H ;
Liu, YP .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1996, 79 (05) :1169-1180
[3]   GRAIN-BOUNDARY RESISTIVITY IN ZIRCONIA-BASED MATERIALS - EFFECT OF SINTERING TEMPERATURES AND IMPURITIES [J].
BADWAL, SPS .
SOLID STATE IONICS, 1995, 76 (1-2) :67-80
[4]  
BADWAL SPS, 1988, MATER SCI FORUM, V34, P195
[5]   Properties of La0.6Sr0.4Co0.2Fe0.8O3-δ (LSCF) double layer cathodes on gadolinium-doped cerium oxide (CGO) electrolytes -: I.: Role of SiO2 [J].
Bae, JM ;
Steele, BCH .
SOLID STATE IONICS, 1998, 106 (3-4) :247-253
[6]   IMPORTANCE OF THE SURFACE EXCHANGE KINETICS AS RATE-LIMITING STEP IN OXYGEN PERMEATION THROUGH MIXED-CONDUCTING OXIDES [J].
BOUWMEESTER, HJM ;
KRUIDHOF, H ;
BURGGRAAF, AJ .
SOLID STATE IONICS, 1994, 72 (pt 2) :185-194
[7]  
Brongersma H H, 1978, Rev Sci Instrum, V49, P707, DOI 10.1063/1.1135598
[8]   A DIFFUSIONAL PHASE-TRANSFORMATION IN ZRO2-4 WT-PERCENT Y2O3 INDUCED BY SURFACE SEGREGATION [J].
CHAIM, R ;
BRANDON, DG ;
HEUER, AH .
ACTA METALLURGICA, 1986, 34 (10) :1933-1939
[9]   Surface cleaning and characterization of yttria-stabilized zirconia [J].
de Ridder, M ;
van Welzenis, RG ;
Brongersma, HH .
SURFACE AND INTERFACE ANALYSIS, 2002, 33 (04) :309-317
[10]   EFFECT OF INTERGRANULAR GLASS-FILMS ON THE ELECTRICAL-CONDUCTIVITY OF 3Y-TZP [J].
GODICKEMEIER, M ;
MICHEL, B ;
ORLIUKAS, A ;
BOHAC, P ;
SASAKI, K ;
GAUCKLER, L ;
HEINRICH, H ;
SCHWANDER, P ;
KOSTORZ, G ;
HOFMANN, H ;
FREI, O .
JOURNAL OF MATERIALS RESEARCH, 1994, 9 (05) :1228-1240