摘要
R&D studies concerning Pb-17Li blankets for DEMO suggest the use of coatings either as tritium permeation barriers for the water cooled blanket or as electrical insulators for the self cooled blanket, The production of coatings resistant to the thermal and mechanical stresses typical of the blanket operating conditions is the target. The present work describes the results of an experimental programme aimed at evaluating the effects of heat treatment and cooling rate on the microstructural and mechanical characteristics of aluminide coatings deposited on MANET steel (DIN 1.4914) by the hot-dipping process. The temperature of the post-deposition heat treatment that allows obtaining structures like FeAl and alpha-Fe(Al), instead of the mon brittle FexAly intermetallics, has been identified. The coatings have been characterized by optical metallography, microhardness measurements, scanning electron microscopy (SEM), energy dispersive X-ray analysis (EDS) and X-ray diffraction on the surface.
引用
收藏
页码:214 / 218
页数:5
相关论文
共 19 条
[1]   FLOW AND FRACTURE OF FE-AL [J].
BAKER, I ;
GAYDOSH, DJ .
MATERIALS SCIENCE AND ENGINEERING, 1987, 96 :147-158
[2]  
BENAMATI G, 1994, RESULTS THERMAL FATI
[3]  
BENAMATI G, 1993, J NUCL MATER, V212, P1557
[4]  
BENAMATI G, 1994, FUS TECH, V2, P1341
[5]   PREPARATION AND CHARACTERIZATION OF AL2O3/FEXALY LAYERS ON MANET STEEL [J].
GLASBRENNER, H ;
BORGSTEDT, HU .
JOURNAL OF NUCLEAR MATERIALS, 1994, 212 (pt B) :1561-1565
[6]  
GLASBRENNER H, 1995, LIQUID METAL SYSTEMS, P95
[7]  
HAWKINS DT, 1973, METALS HDB, V8, P260
[8]   THE STABILITY OF TRITIUM PERMEATION BARRIERS AND THE SELF-HEALING CAPABILITY OF ALUMINIDE COATINGS IN LIQUID PB-17LI [J].
HUBBERSTEY, P ;
SAMPLE, T ;
TERLAIN, A .
FUSION TECHNOLOGY, 1995, 28 (03) :1194-1199
[9]   EFFECT OF COOLING RATE ON HARDNESS OF FEAL AND NIAL [J].
NAGPAL, P ;
BAKER, I .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1990, 21 (08) :2281-2282
[10]   LOW ALUMINUM CONTENT PERMEATION BARRIER COATINGS FOR DIN-1.4914 MARTENSITIC STEEL (MANET) [J].
PERUJO, A ;
SAMPLE, T ;
SERRA, E ;
KOLBE, H .
FUSION TECHNOLOGY, 1995, 28 (03) :1256-1261