Wettability and surface energy of oxidized and hydrogen plasma-treated diamond films

被引:190
作者
Ostrovskaya, L
Perevertailo, V
Ralchenko, V
Dementjev, A
Loginova, O
机构
[1] Inst Superhard Mat, UA-04074 Kiev, Ukraine
[2] Moscow Gen Phys Inst, Moscow 117942, Russia
[3] RRC, Kurchatov Inst, Moscow 123182, Russia
关键词
diamond properties and applications; surface energy; hydrogenation; wettability;
D O I
10.1016/S0925-9635(01)00636-7
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The wettability of CVD diamond films with liquids of different physico-chemical natures (water, glycerin, tin melt) was investigated by measuring the contact angles using the sessile drop method. The translucent diamond films of 0.5-mm thickness were grown in a microwave plasma CVD using CH4-H-2 mixtures as the source gas, and separated from Si substrates. The growth surfaces have been polished to a roughness of Ra less than or equal to 10 nm, and then exposed to microwave hydrogen plasma or thermal oxidation in air at 500 degreesC. Raman and Auger/XPS spectroscopies, optical and atomic force microscopies have been used to characterize the diamond films. Based on the wettability data, the variations in surface energy induced by hydrogenation and oxidation of polycrystalline diamond have been evaluated by the Fowkes equation. The hydrogenation of the films in the plasma essentially increases hydrophobic properties (contact angle for water increases up to theta=93degrees) as compared to oxidation (theta=32degrees). This is attributable to a reduction in a polar component of the surface energy due to hydrogen adsorption-induced reconstruction of the film surface. For comparison, the wettability of HPHT diamond single crystal, diamond ceramics and pyrolytic graphite have been measured and the differences observed will be discussed in this paper. (C) 2002 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:845 / 850
页数:6
相关论文
共 17 条
[1]  
ALESHIN VG, 1990, CHEM DIAMOND SURFACE
[2]   Hydrogen termination and electron emission from CVD diamond surfaces: a combined secondary electron emission, photoelectron emission microscopy, photoelectron yield, and field emission study [J].
Cui, JB ;
Ristein, J ;
Stammler, M ;
Janischowsky, K ;
Kleber, G ;
Ley, L .
DIAMOND AND RELATED MATERIALS, 2000, 9 (3-6) :1143-1147
[3]  
Deryagin B. V., 1989, WATER DISPERSED SYST
[4]  
FOWKES FM, 1965, CHEM PHYSICS INTERFA, P1
[5]   Effect of the acidity ppof aqueous solutions on the wettability of diamond, graphite and pyrocarbon surfaces [J].
Gribanova, EV ;
Zhukov, AN ;
Antonyuk, IE ;
Benndorf, C ;
Baskova, EN .
DIAMOND AND RELATED MATERIALS, 2000, 9 (01) :1-6
[6]   CALCULATION OF SURFACE ENERGIES FOR LOW INDEX PLANES OF DIAMOND [J].
HALICIOGLU, T .
SURFACE SCIENCE, 1991, 259 (1-2) :L714-L718
[7]   A TENSIOMETRIC STUDY OF DIAMOND (111) AND (110) FACES [J].
HANSEN, JO ;
COPPERTHWAITE, RG ;
DERRY, TE ;
PRATT, JM .
JOURNAL OF COLLOID AND INTERFACE SCIENCE, 1989, 130 (02) :347-358
[8]   Atomic and electronic structure of diamond(111) surfaces .2. (2x1) and (root 3x root 3) reconstructions of the clean and hydrogen-covered three dangling-bond surfaces [J].
Kern, G ;
Hafner, J ;
Kresse, G .
SURFACE SCIENCE, 1996, 366 (03) :464-482
[9]   Wettability of diamond by liquid pure tin [J].
Nogi, K ;
Nishikawa, M ;
Fujii, H ;
Hara, S .
ACTA MATERIALIA, 1998, 46 (07) :2305-2311
[10]  
PEREVERTAILO VM, 1999, P 4 INT S DIAM FILMS, P197