In situ synchrotron SAXS/WAXD studies during melt spinning of modified carbon nanofiber and isotactic polypropylene nanocomposite

被引:20
作者
Ran, SF
Burger, C
Sics, I
Yoon, K
Fang, DF
Kim, KS
Avila-Orta, C
Keum, J
Chu, B [1 ]
Hsiao, BS
Cookson, D
Shultz, D
Lee, M
Viccaro, J
Ohta, Y
机构
[1] SUNY Stony Brook, Dept Chem, Stony Brook, NY 11794 USA
[2] Argonne Natl Lab, Adv Photon Source, ChemMat CARS, Argonne, IL 60439 USA
[3] Toyobo Res Ctr Co Ltd, Shiga 5200292, Japan
关键词
carbon nanofiber; polypropylene; nanocomposite; fiber spinning; SAXS; WAXD;
D O I
10.1007/s00396-004-1125-0
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The structural development of a nanocomposite, containing 95 wt% isotactic polypropylene (iPP) and 5 wt% modified carbon nanofiber (MCNF), during fiber spinning was investigated by in situ synchrotron small-angle X-ray scattering (SAXS) and wide-angle X-ray diffraction (WAXD) techniques. The modification of carbon nanofibers (CNFs) was accomplished by a chemical surface treatment using in situ polymerization of olefin segments to enhance its compatibility with iPP, where the iPP/MCNF nanocomposite was prepared by twostep blending to ensure the dispersion of MCNF. X-ray results showed that at low spin-draw ratios, the iPP/MCNF nanocomposite fiber exhibited much higher iPP crystalline orientation than the control iPP fiber. At higher spin-draw ratios, the crystalline orientation of the nanocomposite fiber and that of the pure iPP fiber was about the same. The crystallinity of the composite fiber was higher than that of the control iPP fiber, indicating the nucleating effect of the modified carbon nanofibers. The nanocomposite fiber also showed larger long periods at low spin-draw ratios. Measurements of mechanical properties indicated that the nanocomposite fiber with 5 wt% MCNF had much higher tensile strength, modulus and longer elongation to break. The mechanical enhancement can be attributed to the dispersion of MCNF in the matrix, which was confirmed by SEM results.
引用
收藏
页码:802 / 809
页数:8
相关论文
共 26 条
[1]  
Alexander LE., 1969, XRAY DIFFRACTION POL
[2]  
Baker R.T.K., 1978, CHEM PHYS CARBON, V14, P83
[3]   Accurate structural control and block formation in the living polymerization of 1,3-dienes by nitroxide-mediated procedures [J].
Benoit, D ;
Harth, E ;
Fox, P ;
Waymouth, RM ;
Hawker, CJ .
MACROMOLECULES, 2000, 33 (02) :363-370
[4]   Rheological behavior of (Short) carbon fiber/thermoplastic composites. Part 1: The influence of fiber type, processing conditions and level of incorporation [J].
Carneiro, OS ;
Maia, JM .
POLYMER COMPOSITES, 2000, 21 (06) :960-969
[5]   Dissolution of full-length single-walled carbon nanotubes [J].
Chen, J ;
Rao, AM ;
Lyuksyutov, S ;
Itkis, ME ;
Hamon, MA ;
Hu, H ;
Cohn, RW ;
Eklund, PC ;
Colbert, DT ;
Smalley, RE ;
Haddon, RC .
JOURNAL OF PHYSICAL CHEMISTRY B, 2001, 105 (13) :2525-2528
[6]   Solution properties of single-walled carbon nanotubes [J].
Chen, J ;
Hamon, MA ;
Hu, H ;
Chen, YS ;
Rao, AM ;
Eklund, PC ;
Haddon, RC .
SCIENCE, 1998, 282 (5386) :95-98
[7]  
Curran SA, 1998, ADV MATER, V10, P1091, DOI 10.1002/(SICI)1521-4095(199810)10:14<1091::AID-ADMA1091>3.0.CO
[8]  
2-L
[9]  
Dresselhaus M. S. G., 1988, SPRINGER SERIES MAT, V5
[10]  
FRIEND SO, 1997, Patent No. 5611964