Microscopic visualization on crystalline morphologies of thin films for poly[(R)-3-hydroxybutyric acid] and its copolymer

被引:61
作者
Abe, H [1 ]
Kikkawa, Y
Iwata, T
Aoki, H
Akehata, T
Doi, Y
机构
[1] RIKEN, Inst Phys & Chem Res, Polymer Chem Lab, Wako, Saitama 3510198, Japan
[2] Sci Univ Tokyo, Dept Ind Chem, Shinjuku Ku, Tokyo 1628601, Japan
关键词
poly[(R)-3-hydroxybutyric acid; thin film; lamellar morphology;
D O I
10.1016/S0032-3861(99)00231-1
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Thin films with average layer thickness 100 nm of poly[(R)-3-hydroxybutyric acid] (P[(R)-3HB]) and poly[(R)-3-hydroxybutyric acid-co-10 mol% 6-hydroxyhexanoic acid] were isothermally crystallized at a given crystallization temperature after melting at 200 degrees C. The spherulitic and lamellar morphologies of polyester thin films were investigated by means of optical microscopy, transmission electron microscopy and atomic force microscopy. After isothermal crystallization, the uniform two-dimensional spherulites which have the stacking texture of flat-on lamellae were developed throughout both polyester thin films. Each flat-on crystal gave a well-resolved electron diffractogram, and all electron diffractograms were identical. Accordingly, the 6-hydroxyhexanoic acid units were rejected from the tightly packed region of lamellar crystals. Both the lamellar periodicity and lamellar width of polyester thin films increased with a rise in the crystallization temperature. At the growth front of crystalline lamellae, microfibril crystals with 30-50 nm width were present. The enzymatic hydrolysis of thin films was carried out at 25 degrees C using an aqueous solution of PHB depolymerase from Alcaligenes faecalis. After enzymatic degradation, the jagged texture along the crystal long-axis could be observed at the ends of crystalline lamellae on the surface of the thin films. These observations suggest that the lamellar crystals of P[(R)-3HB] is composed of both tight molecular packing regions of microfibril crystals and loose molecular packing boundary regions. (C) 1999 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:867 / 874
页数:8
相关论文
共 27 条
  • [1] PHYSICAL-PROPERTIES AND ENZYMATIC DEGRADABILITY OF COPOLYMERS OF (R)-3-HYDROXYBUTYRIC AND 6-HYDROXYHEXANOIC ACIDS
    ABE, H
    DOI, Y
    AOKI, H
    AKEHATA, T
    HORI, Y
    YAMAGUCHI, A
    [J]. MACROMOLECULES, 1995, 28 (23) : 7630 - 7637
  • [2] Solid-state structures and enzymatic degradabilities for melt-crystallized films of copolymers of (R)-3-hydroxybutyric acid with different hydroxyalkanoic acids
    Abe, H
    Doi, Y
    Aoki, H
    Akehata, T
    [J]. MACROMOLECULES, 1998, 31 (06) : 1791 - 1797
  • [3] ABE H, 1997, POLYMER, V39, P59
  • [4] OCCURRENCE, METABOLISM, METABOLIC ROLE, AND INDUSTRIAL USES OF BACTERIAL POLYHYDROXYALKANOATES
    ANDERSON, AJ
    DAWES, EA
    [J]. MICROBIOLOGICAL REVIEWS, 1990, 54 (04) : 450 - 472
  • [5] CRYSTALLIZATION AND MORPHOLOGY OF A BACTERIAL THERMOPLASTIC - POLY-3-HYDROXYBUTYRATE
    BARHAM, PJ
    KELLER, A
    OTUN, EL
    HOLMES, PA
    [J]. JOURNAL OF MATERIALS SCIENCE, 1984, 19 (09) : 2781 - 2794
  • [6] MORPHOLOGY OF SINGLE-CRYSTALS OF POLY(HYDROXYBUTYRATE) AND COPOLYMERS OF HYDROXYBUTYRATE AND HYDROXYVALERATE
    BIRLEY, C
    BRIDDON, J
    SYKES, KE
    BARKER, PA
    ORGAN, SJ
    BARHAM, PJ
    [J]. JOURNAL OF MATERIALS SCIENCE, 1995, 30 (03) : 633 - 638
  • [7] CRYSTALLIZATION PHENOMENA IN BACTERIAL POLY[(R)-3-HYDROXYBUTYRATE] .3. TOUGHENING VIA TEXTURE CHANGES
    DEKONING, GJM
    SCHEEREN, AHC
    LEMSTRA, PJ
    PEETERS, M
    REYNAERS, H
    [J]. POLYMER, 1994, 35 (21) : 4598 - 4605
  • [8] DOI Y, 1990, MACROMOLECULES, V23, P26, DOI 10.1021/ma00203a006
  • [9] DOI Y, 1995, MACROMOLECULES, V28, P4822, DOI 10.1021/ma00118a007
  • [10] DOI Y, 1988, APPL MICROBIOL BIOT, V28, P330, DOI 10.1007/BF00268190