Syntheses, structures, physical properties, and theoretical studies of CeMxOS (M = Cu, Ag; x ≈ 0.8) and CeAgOS

被引:43
作者
Chan, George H.
Deng, Bin
Bertoni, Mariana
Ireland, John R.
Hersam, Mark C.
Mason, Thomas O.
Van Duyne, Richard P.
Ibers, James A.
机构
[1] Northwestern Univ, Dept Chem, Evanston, IL 60208 USA
[2] Northwestern Univ, Dept Mat Sci & Engn, Evanston, IL 60208 USA
关键词
D O I
10.1021/ic061041k
中图分类号
O61 [无机化学];
学科分类号
070301 ; 081704 ;
摘要
Black single crystals of the two nonstoichiometric cerium coinage-metal oxysulfide compounds CeCuxOS and CeAgxOS (x approximate to 0.8) have been prepared by the reactions of Ce2S3 and CuO or Ag2O at 1223 or 1173 K, respectively. A black powder sample of CeAgOS has been prepared by the stoichiometric reaction of Ce2S3, CeO2, Ag2S, and Ag at 1073 K. These isostructural materials crystallize in the ZrSiCuAs structure type with two formula units in the tetragonal space group P4/nmm. Refined crystal structure results and chemical analyses provide evidence that the previously known anomalously small unit-cell volume of LnCuOS for Ln = Ce (Ln = rare-earth metal) is the result of Cu vacancies and the concomitant presence of both Ce3+ and Ce4+. Both CeCu0.8OS and CeAgOS are paramagnetic with mu(eff) values of 2.13(6) and 2.10(1) mu(B), respectively. CeCu0.8OS is a p-type semiconductor with a thermal activation energy E-a = 0.22 eV, sigma(electrical) = 9.8(1) 10(-3) S/cm at 298 K, and an optical band gap E-g < 0.73 eV. CeAgOS has conductivity sigma(conductivity) = 0.16(4) S/cm and an optical band gap E-g = 0.71 eV at 298 K. Theoretical calculations with an on-site Coulomb repulsion parameter indicate that the Ce 4f states are fully spin-polarized and are not localized in CeCuOS, CeCu0.75OS, or CeAgOS. Calculated band gaps for CeCu0.75OS and CeAgOS are 0.6 and 0.8 eV, respectively.
引用
收藏
页码:8264 / 8272
页数:9
相关论文
共 41 条
[1]   Relationship between bond valence and bond softness of alkali halides and chalcogenides [J].
Adams, S .
ACTA CRYSTALLOGRAPHICA SECTION B-STRUCTURAL SCIENCE CRYSTAL ENGINEERING AND MATERIALS, 2001, 57 (57) :278-287
[2]   CRYSTAL-STRUCTURE AND CONDUCTIVITY OF THE NEW SUPERIONIC CONDUCTOR AG4HF3S8 [J].
AMIEL, O ;
WADA, H .
JOURNAL OF SOLID STATE CHEMISTRY, 1995, 115 (01) :112-119
[3]  
[Anonymous], 1998, BIOELECTROMAGNETICS
[4]  
Blaha P, 2001, WIEN2K AUGMENTED PLA
[5]   BOND-VALENCE PARAMETERS OBTAINED FROM A SYSTEMATIC ANALYSIS OF THE INORGANIC CRYSTAL-STRUCTURE DATABASE [J].
BROWN, ID ;
ALTERMATT, D .
ACTA CRYSTALLOGRAPHICA SECTION B-STRUCTURAL SCIENCE, 1985, 41 (AUG) :244-247
[6]  
*BRUK AN XRAY INST, 2003, SMART VERS 5 054 DAT
[7]   CRYSTAL-STRUCTURE OF CERIUM BISMUTH OXYSULFIDE [J].
CEOLIN, R ;
RODIER, N .
ACTA CRYSTALLOGRAPHICA SECTION B-STRUCTURAL SCIENCE, 1976, 32 (MAY15) :1476-1479
[8]  
Charkin DO, 1999, RUSS J INORG CHEM+, V44, P833
[9]   LOCAL-DENSITY FUNCTIONAL AND ON-SITE CORRELATIONS - THE ELECTRONIC-STRUCTURE OF LA2CUO4 AND LACUO3 [J].
CZYZYK, MT ;
SAWATZKY, GA .
PHYSICAL REVIEW B, 1994, 49 (20) :14211-14228
[10]   KAg5S3 [J].
Emirdag, M ;
Schimek, GL ;
Kolis, JW .
ACTA CRYSTALLOGRAPHICA SECTION C-CRYSTAL STRUCTURE COMMUNICATIONS, 1998, 54 :1376-1378