Development of porosity upon chemical activation of kraft lignin with ZnCl2

被引:117
作者
GonzalezSerrano, E [1 ]
Cordero, T [1 ]
RodriguezMirasol, J [1 ]
Rodriguez, JJ [1 ]
机构
[1] UNIV MALAGA,DEPT CHEM ENGN,E-29071 MALAGA,SPAIN
关键词
D O I
10.1021/ie970261q
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
Chemical activation of kraft lignin with. ZnCl2 allows one to obtain high surface area activated carbons with a predominantly microporous structure. Most of porosity develops within the thermal range of 400-500 degrees C, where an increase of temperature leads to increasing micropore volume values (up to approximate to 1 cm(3)/g) and a wider distribution of micropore size. An increasing mesoporositiy is also observed. Increasing the impregnation ratio (ZnCl2/lignin, wt) has a similar effect on the evolution of the porous structure. The mesopore distribution remains within the low-size range even at high impregnation ratios (up to 2.3). At 500 degrees C and an impregnation ratio of 2.3, where the highest contribution of mesoporosity was observed, the mesopore volume reached a value of 0.59 cm(3)/g. These conditions allowed us to obtain a BET surface area of 1800 m(2)/g, including the external or non-microporous surface of 200 m(2)/g. The porous structure developed suggests a fairly homogeneous distribution of the activating agent favored by the softening and partial fusion which kraft lignin undergoes within the temperature range of 180-280 degrees C.
引用
收藏
页码:4832 / 4838
页数:7
相关论文
共 21 条