Cracking behaviour of PVD tungsten coatings deposited on steel substrates

被引:55
作者
Ganne, T
Crépin, M
Serror, S
Zaoui, A [1 ]
机构
[1] Ecole Polytech, CNRS, Mecan Solides Lab, F-91128 Palaiseau, France
[2] Ctr Tech Arcueil, F-94114 Arcueil, France
关键词
magnetron sputtering; residual stresses; crystallographic texture; critical cracking stress; tungsten; coating;
D O I
10.1016/S1359-6454(02)00256-2
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Tungsten coatings have been deposited on steel substrates by magnetron sputtering. For the same processing conditions, the increase of the coating thickness enhances the (111) component of the crystallographic texture whereas the residual stress level decreases. Tensile and four-point bending tests, associated with an acoustic emission analysis, have been performed inside a SEM chamber in order to study the cracking mechanisms. When the residual stresses are taken into account, an intrinsic critical cracking stress and the associated energy release rate can be determined; the obtained values suggest an intergranular cracking mechanism. No debonding has been observed at the interface despite the large plastic deformation of the substrate at the crack tips. The observed strain localisation modes in the substrate near the interface have been shown to have a major influence on the limit crack density. (C) 2002 Acta Materialia Inc. Published by Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:4149 / 4163
页数:15
相关论文
共 26 条
[1]   EXPERIMENTAL CHARACTERIZATION OF THE LOCAL STRAIN FIELD IN A HETEROGENEOUS ELASTOPLASTIC MATERIAL [J].
ALLAIS, L ;
BORNERT, M ;
BRETHEAU, T ;
CALDEMAISON, D .
ACTA METALLURGICA ET MATERIALIA, 1994, 42 (11) :3865-3880
[2]   Measurement of Young's modulus, hardness acid flow stress of coatings by a depth-sensing indentation instrument. [J].
Angelelis, C ;
Felder, E ;
Farges, G ;
Jauberteau, I ;
Nadal, M .
ANNALES DE CHIMIE-SCIENCE DES MATERIAUX, 1998, 23 (5-6) :829-846
[3]  
[Anonymous], 1995, MECANIQUE RUPTURE
[4]  
BRANDES EA, SMITHELLS MAT REFERE
[5]   Low cycle fatigue behaviour of β treated zirconium:: Partial irreversibility of twinning and consequences for damage [J].
Crépin, J ;
Bretheau, T ;
Caldemaison, D ;
Ferrer, F .
ACTA MATERIALIA, 2000, 48 (02) :505-516
[6]   ION-BEAM-INDUCED TEXTURE FORMATION IN VACUUM-CONDENSED THIN METAL-FILMS [J].
DOBREV, D .
THIN SOLID FILMS, 1982, 92 (1-2) :41-53
[7]   Study of the fragile-to-ductile transition of tungsten [J].
Farre, J ;
Lamaison, M ;
Cosculluela, A ;
Lataillade, JL .
JOURNAL DE PHYSIQUE IV, 1997, 7 (C3) :879-884
[8]  
Francois D., 1998, VISCOPLASTICITY DAMA, Vvol 2
[9]  
GERGAUD P, 1992, THESIS ECOLE NATL SU
[10]   Mechanical properties of W and W(C) thin films: Young's modulus, fracture toughness and adhesion [J].
Harry, E ;
Rouzaud, A ;
Ignat, M ;
Juliet, P .