Formation and environmental stability of nanocrystalline and amorphous hydrides in the 2Mg-Fe mixture processed by controlled reactive mechanical alloying (CRMA)

被引:51
作者
Varin, RA
Li, S
Calka, A
Wexler, D
机构
[1] Univ Waterloo, Dept Mech Engn, Waterloo, ON N2L 3G1, Canada
[2] Univ Wollongong, Dept Mat Sci & Engn, Wollongong, NSW 2518, Australia
基金
加拿大自然科学与工程研究理事会;
关键词
hydrogen storage materials; nanostructured and amorphous hydrides; reactive mechanical alloying; X-ray diffraction; thermal analysis and calorimetry;
D O I
10.1016/j.jallcom.2003.11.015
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The synthesis of the Mg2FeH6 complex hydride has been attempted by controlled reactive mechanical alloying (CRMA) of 2Mg-Fe powder mixture under hydrogen using shearing mode in a magneto-mill Uni-Ball-Mill 5. The first batch of 2Mg-Fe powder was initially mechanically pre-alloyed by milling under argon with the addition of small amount of toluene and subsequently reactively milled under hydrogen. The second batch was directly milled under hydrogen. No formation of Mg2FeH6 has been observed even after the longest milling duration of 59 h. In the powders reactively alloyed directly under hydrogen some quantity of nanocrystalline beta-MgH2 hydride was formed during the first 10-15 h of milling. However, the X-ray diffraction (XRD) peaks due to beta-MgH2 disappeared after further milling up to 59 h. In addition, the XRD peaks corresponding to the nanocrystalline Mg completely disappeared after 20-24 h of CRMA under hydrogen in both batches of powders while strong but broadened peaks from Fe were still visible. The absorption of hydrogen from the milling vial occurred continuously up to 20-24 h of milling. Energy dispersive spectroscopy (EDS) analysis clearly showed that Mg was still present in the microstructure of powder particles after milling up to 59 h for both batches of 2Mg-Fe powder. These results clearly indicate that amorphous Mg and amorphous hydrides are being formed after prolonged CRMA under shearing mode. It has been shown for the first time that beta-MgH2 undergoes hydrolysis into Mg(OH)(2) when it is exposed for several months to the moisture in the environment. This is associated with abnormally high weight losses (similar to10 wt.%) measured by thermogravimetric analysis (TGA) and the appearance of two endothermic differential scanning calorimetry (DSC) peaks related to the desorption of hydrogen from beta-MgH2 and release of water from Mg(OH)(2). Other powders after prolonged milling showed TGA weight losses on the order of 2-4 wt.% and only a single DSC peak, which provides additional strong evidence that amorphous hydrides were formed during CRMA. During DSC tests up to 500degreesC the amorphous Mg crystallized into the nanocrystalline Mg phase. (C) 2003 Elsevier B.V. All rights reserved.
引用
收藏
页码:270 / 286
页数:17
相关论文
共 23 条
  • [1] UNIVERSAL HIGH-PERFORMANCE BALL-MILLING DEVICE AND ITS APPLICATION FOR MECHANICAL ALLOYING
    CALKA, A
    RADLINSKI, AP
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1991, 134 : 1350 - 1353
  • [2] CALKA A, Patent No. 5383615
  • [3] CALKA A, Patent No. 9104810
  • [4] CALKA A, 2001, P INT S PROC FABR AD, V9, P263
  • [5] Synthesis of Mg2FeH6 by reactive mechanical alloying:: formation and decomposition properties
    Gennari, FC
    Castro, FJ
    Gamboa, JJA
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2002, 339 (1-2) : 261 - 267
  • [6] Thermal decomposition behaviour of polyamide fire-retardant compositions containing magnesium hydroxide filler
    Hornsby, PR
    Wang, J
    Rothon, R
    Jackson, G
    Wilkinson, G
    Cossick, K
    [J]. POLYMER DEGRADATION AND STABILITY, 1996, 51 (03) : 235 - 249
  • [7] Direct synthesis of Mg2FeH6 by mechanical alloying
    Huot, J
    Boily, S
    Akiba, E
    Schulz, R
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 1998, 280 (1-2) : 306 - 309
  • [8] Magnesium-based nanocomposites chemical hydrides
    Huot, J
    Liang, G
    Schulz, R
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2003, 353 (1-2) : L12 - L15
  • [9] *INT CTR DIFFR DAT, 1997, 120697 PDF INT CTR D
  • [10] *INT CTR DIFFR DAT, 1997, 380843 PDF INT CTR D