Microstructure of Al3Sc with ternary transition-metal additions

被引:192
作者
Harada, Y [1 ]
Dunand, DC [1 ]
机构
[1] Northwestern Univ, Dept Mat Sci & Engn, Evanston, IL 60208 USA
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2002年 / 329卷
基金
日本学术振兴会; 美国能源部;
关键词
Ll(2)-trialuminides; microstructure; lattice parameter; microhardness;
D O I
10.1016/S0921-5093(01)01608-2
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The microstructure of binary Al3Sc and ternary Al-3(S1-yXy), where X is one of the transition metals from Group IIIA (Y) lIVA (Ti, Zr or Hf) or VA (V, Nb or Ta), was investigated as a function of alloying element concentration for 0.1 less than or equal to y less than or equal to 0.75. Alloys with Group IIIA and IVA additions exhibited a single Ll(2) solid-solution phase with some Kirkendall porosity. At the highest concentration studied, a second phase precipitated with the D0(19) (Y), D0(22) (Ti) or D0(23) (Zr and Hf) structure. Conversely, alloys with Group VA additions exhibited both the Ll(2) trialuminide phase and a dendritic trialuminide second phase with D0(22) structure for all concentrations studied. The solubility limit in the ternary Ll(2)-type Al-3(Sc1-yXy) phase was high for Group IIIA and IVA metals (almost 12.5 at.% or y = 0.5), and much lower for Group VA metals (from about 1.8 at.% or y = 0.07 for Ta to about 2.7 at.% or y = 0.11 for V). Similarly, the solubility limit of Sc in the non-Ll(2). phases decreases from the Group IIIA trialuminide to the Group VA trialuminides. The lattice parameter of the Ll(2) solid-solution decreased linearly with increasing concentration of Group IVA and VA metals, but increased linearly with concentration of Y (Group IIIA). This linear concentration dependence of the lattice parameter is found to correlate with the atomic size mismatch between Sc and the transition metal. The microhardness of the Ll(2) solid-solution increased linearly with increasing concentration of ternary elements. The concentration dependence of hardness is strongest for Group VA metals and weakest for Group IVA metals, for which a correlation is found with the concentration dependence of lattice parameter. (C) 2002 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:686 / 695
页数:10
相关论文
共 23 条
[1]   FORMATION OF METASTABLE LL2-AL3Y THROUGH RAPID SOLIDIFICATION PROCESSING [J].
FOLEY, JC ;
PEREPEZKO, JH ;
SKINNER, DJ .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1994, 179 :205-209
[2]  
Fukunaga K, 1997, MAT SCI ENG A-STRUCT, V240, P202
[3]   Creep properties of coarse-grained Al(Sc) alloys at 300°C [J].
Fuller, CB ;
Seidman, DN ;
Dunand, DC .
SCRIPTA MATERIALIA, 1999, 40 (06) :691-696
[4]   DEFORMATION AND FRACTURE OF L12 TRIALUMINIDES [J].
GEORGE, EP ;
POPE, DP ;
FU, CL ;
SCHNEIBEL, JH .
ISIJ INTERNATIONAL, 1991, 31 (10) :1063-1075
[5]  
GUARD RW, 1959, T AM I MIN MET ENG, V215, P807
[6]   Carbon effects in rapidly solidified Ni3Al [J].
Huang, S. C. ;
Briant, C. L. ;
Chang, K. -M. ;
Taub, A. I. ;
Hall, E. L. .
JOURNAL OF MATERIALS RESEARCH, 1986, 1 (01) :60-67
[7]  
Kita I., 1995, High-Temperature Ordered Intermetallic Alloys VI. Symposium, P1241
[8]  
MASSALSKI TB, 1986, BINARY ALLOY PHASE D, P161
[9]   FORMATION OF TERNARY L12 COMPOUNDS IN AL3TI-BASE ALLOYS [J].
NAKAYAMA, Y ;
MABUCHI, H .
INTERMETALLICS, 1993, 1 (01) :41-48
[10]  
NICHOLSON DM, 1991, MATER RES SOC SYMP P, V186, P229