Coarse blast furnace slag as a cementitious material, comparative study as a partial replacement of Portland cement and as an alkali activated cement

被引:67
作者
Escalante-Garcia, J. I. [1 ]
Espinoza-Perez, L. J. [1 ]
Gorokhovsky, A. [1 ]
Gomez-Zamorano, L. Y. [2 ]
机构
[1] Ceram Engn Grp, Unidad Saltillo, Inst Politecn Nacl, Ctr Invest & Estudios Avanzados, Saltillo 25900, Coahuila, Mexico
[2] Univ Autonoma Nuevo Leon, FIME, San Nicolas De Los Garza 66451, Nuevo Leon, Mexico
关键词
Concrete; Blast furnace slag; Blended cements; Alkaline activation; Strength; Microstructure; HYDRATION PRODUCTS; REACTIVITY; STRENGTH;
D O I
10.1016/j.conbuildmat.2009.02.002
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
The cementitious performance of a coarse granulated blast furnace slag, 2900 cm(2)/g, was investigated in concretes of 230. 280 and 330 kg binder/m(3). First, the slag partially replaced 30%, 50% and 70% of Portland cement, the strength reduced as the amount Of slag increased; however, for high binder contents, similar strengths were attained for lower Portland cement contents. Second, the slag was alkali activated with sodium silicate (moduli 1.7 and 2) at 4%, 6% and 8% %Na2O, the strength increased with the amount of slag in the concrete and developed faster as %Na2O increased. The microstructures of both type of concretes were dense: however, the strengths of activated slag were superior at similar binder loads, indicating that the hydration products of activated slag are of higher intrinsic strength. (C) 2009 Elsevier Ltd. All rights reserved.
引用
收藏
页码:2511 / 2517
页数:7
相关论文
共 23 条
[1]  
[Anonymous], 1991, 2111 ACI
[2]  
[Anonymous], 1995, ANN BOOK ASTM STAND, DOI DOI 10.1520/2002C
[3]  
*ASTM, 1995, C14390A ASTM
[4]  
DAUBE J, 1986, ASTM STP, V897, P5
[5]   Cementitious composites of pulverised fuel ash and blast furnace slag activated by sodium silicate:: effect of Na2O concentration and modulus [J].
Escalante Garcia, J. I. ;
Campos-Venegas, K. ;
Gorokhovsky, A. ;
Fernandez, A. .
ADVANCES IN APPLIED CERAMICS, 2006, 105 (04) :201-208
[6]   Admixture of a geothermal waste to alkali activated blast furnace slag [J].
Escalante, JI ;
Mendoza, G ;
Mancha, H ;
Fuentes, AF ;
Bustos, JL ;
Gómez-Zamorano, LY .
BOLETIN DE LA SOCIEDAD ESPANOLA DE CERAMICA Y VIDRIO, 2002, 41 (06) :539-544
[7]   Reactivity of blast-furnace slag in Portland cement blends hydrated under different conditions [J].
Escalante, JI ;
Gómez, LY ;
Johal, KK ;
Mendoza, G ;
Mancha, H ;
Méndez, J .
CEMENT AND CONCRETE RESEARCH, 2001, 31 (10) :1403-1409
[8]   Nonevaporable water from neat OPC and replacement materials in composite cements hydrated at different temperatures [J].
Escalante-Garcia, JI .
CEMENT AND CONCRETE RESEARCH, 2003, 33 (11) :1883-1888
[9]   Hydration products and reactivity of blast-furnace slag activated by various alkalis [J].
Escalante-García, JI ;
Fuentes, AF ;
Gorokhovsky, A ;
Fraire-Luna, PE ;
Mendoza-Suarez, G .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2003, 86 (12) :2148-2153
[10]   Reactivity and mechanical properties of alkali activated blast furnace slag [J].
Escalante-Garcia, JI ;
Méndez-Nonell, J ;
Gorokhovsky, A ;
Fraire-Luna, PE ;
Mancha-Molinar, H ;
Mendoza-Suarez, G .
BOLETIN DE LA SOCIEDAD ESPANOLA DE CERAMICA Y VIDRIO, 2002, 41 (05) :451-458