Oxygen and carbon dioxide kinetic challenges for thermophilic mineral bioleaching processes

被引:23
作者
de Kock, SH [1 ]
Barnard, P [1 ]
du Plessis, CA [1 ]
机构
[1] BHP Billiton, Johannesburg Technol Ctr, ZA-2125 Randburg, South Africa
关键词
Archaea; bioleaching; carbon dioxide; oxygen; Sulfolobus; thermophilic;
D O I
10.1042/BST0320273
中图分类号
Q5 [生物化学]; Q7 [分子生物学];
学科分类号
071010 ; 081704 ;
摘要
Agitated bacterial tank bioleaching reactors are currently sparged with air to satisfy both oxygen and CO(2) requirements of microbial cells. Under high-sulphide loading conditions, as is the case with high-grade metal sulphide concentrates, the microbial and chemical demand for oxygen is significantly increased during the bioleaching process. Sparging with enriched oxygen gas may offer an alternative process option to increased agitation and sparged aeration, to overcome the mass transfer difficulties at elevated temperatures where thermophilic Archaea, rather than Bacteria, are used. In the case of air sparging, the Do (dissolved oxygen) concentration in tank reactors could not be increased to a point where it would become inhibitory due to the limited oxygen content of air (20.9% O(2)). The use of enriched oxygen in such reactors at large scale does, however, pose its own set of process risks. The first aim of this investigation was, therefore, to determine the effects of various DO concentrations, in both the limiting and inhibitory ranges, on the microbial activity of Sulfolobus sp. U40813, a typical thermophilic mineral-leaching archaeon. Secondly, the effect of CO(2) concentration on the rate of ferrous iron oxidation was investigated. Both the oxygen and CO(2) kinetics were examined in controlled batch cultures at 78degreesC, using ferrous sulphate and potassium tetrathionate as energy sources. The optimal DO concentration for iron oxidation was found to be between 1.5 and 4.1 mg . 1(-1). The use of elevated DO concentrations (above 4.1 mg . 1-1) inhibited the ferrous oxidation rates. The optimal gas CO(2) concentration for ferrous iron oxidation was found to be in the range 7-17% (v/v). The iron oxidation rates were, however, severely limited at CO(2) Concentrations less than 7%, indicating that the CO(2) Supply was limiting in this range and inhibited the microbial growth rate.
引用
收藏
页码:273 / 275
页数:3
相关论文
共 5 条
  • [1] MARSH RM, 1983, PROGR BIOHYDROMETALL, P71
  • [2] AUTOTROPHIC GROWTH AND INORGANIC SULFUR COMPOUND OXIDATION BY SULFOLOBUS SP IN CHEMOSTAT CULTURE
    NIXON, A
    NORRIS, PR
    [J]. ARCHIVES OF MICROBIOLOGY, 1992, 157 (02) : 155 - 160
  • [3] NORRIS P, 1989, FEMS SYMP, V49, P24
  • [4] Norris P.R., 1989, Biohydrometallurgy 1989, P3
  • [5] Rawlings DE, 1997, BIOMINING THEORY MIC