High temperature deformation of precursor-derived amorphous Si-B-C-N ceramics

被引:49
作者
Baufeld, B
Gu, H
Bill, J
Wakai, F
Aldinger, F
机构
[1] Max Planck Inst Met Forsch, Stuttgart, Germany
[2] Univ Stuttgart, Inst Nichtmet Anorgan Mat, D-7000 Stuttgart, Germany
[3] Japan Sci & Technol Corp, JST, ICORP, Ceram Superplast Project, Nagoya, Aichi, Japan
关键词
precursors-organic; porosity; mechanical properties; plasticity; amorphous ceramics; Si-B-C-N;
D O I
10.1016/S0955-2219(99)00079-5
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The deformation of amorphous Si-B-C-N ceramics derived from polymeric boron-containing polysilylcarbodi-imide was investigated at temperatures between 1500 and 1700 degrees C in nitrogen atmosphere. The composition of the as-thermolysed ceramic was determined to be SiB0.41+/-0.11C3.39+/-0.44N2.42+/-0.31 O0.22+/-0.14 and no remarkable change was observed after testing at 1600 degrees C in nitrogen atmosphere. Under uniaxial compression a true strain of more than 30% was achieved without visible damage. By compression at constant strain rate a maximum densification of 26% was achieved. Besides densification non-Newtonian viscous flow was observed with an apparent activation energy of 0.8 MJ mol(-1) and an apparent activation volume between 2.5 and 0.2 nm(3). A free volume in the same order of a few cubic nanometers was assumed. At 1600 degrees C the amorphous ceramic starts to crystallize with a volume fraction of crystalline phase less than 10% after several hours. The apparent increase in stress during deformation was explained by changes in sample size, porosity and intrinsic structure due to a decrease in free volume. (C) 1999 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:2797 / 2814
页数:18
相关论文
共 70 条
[1]  
An LA, 1998, J AM CERAM SOC, V81, P1349
[2]  
Baldus H.-P., 1997, Angewandte Chemie (International Edition in English), V36, P328, DOI 10.1002/anie.199703281
[3]  
BALDUS HP, 1992, MATER RES SOC SYMP P, V271, P821, DOI 10.1557/PROC-271-821
[4]  
BAUFELD B, 1998, 6 INT S CER MAT COMP, P277
[5]  
Bill J, 1998, PHYS STATUS SOLIDI A, V166, P269, DOI 10.1002/(SICI)1521-396X(199803)166:1<269::AID-PSSA269>3.0.CO
[6]  
2-7
[7]  
Bill J, 1996, Z METALLKD, V87, P827
[8]   PRECURSOR-DERIVED COVALENT CERAMICS [J].
BILL, J ;
ALDINGER, F .
ADVANCED MATERIALS, 1995, 7 (09) :775-&
[9]  
BILL J, 1994, MATER RES SOC SYMP P, V346, P605, DOI 10.1557/PROC-346-605
[10]  
BILL J, 1995, ADV SCI TECHNOL B, V3, P1291