NaCl-induced hot corrosion of Fe-Mn-Al-C alloys

被引:71
作者
Wang, CJ [1 ]
Chang, YC [1 ]
机构
[1] Natl Taiwan Univ Sci & Technol, Dept Engn Mech, Sect 4, Taipei 10617, Taiwan
关键词
Fe-Mn-Al-C alloys; hot corrosion; NaCl; Al2O3;
D O I
10.1016/S0254-0584(01)00515-6
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The purpose of this study is to investigate the hot corrosion behavior of three Fe-30.1Mn-6.93Al-0.86C base alloys with different aluminum and chromium contents. The hot corrosion experiments were performed at a temperature range from 750 to 850degreesC in air with 2 mg cm(-2) NaCl deposit. The performance of alloys and hot corrosion mechanism were determined by the results of weight change kinetics and subscale analyses. The results show that NaCl accelerated the oxidation of Fe-Mn-Al-C alloys. The hot corrosion behavior depends on the environment temperature and the contents of aluminum and chromium. When the aluminum content exceeds 8 wt.%, the Al2O3 scale forms in simple oxidation. The addition of chromium gives the best oxidation resistance at both 750 and 800degreesC. In hot corrosion environments, the addition of chromium reduced the metal loss but did not improve the overall hot corrosion resistance. A higher aluminum content is beneficial for the alloy to form Al2O3 at 850degreesC, resulting in the best corrosion resistance in this study. (C) 2002 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:151 / 161
页数:11
相关论文
共 20 条
[1]   HIGH-TEMPERATURE OXIDATION OF FE-31MN-9AL-0CR-0.87C, 3CR-0.87C, AND 6CR-0.87C ALLOYS [J].
DUH, JG ;
WANG, CJ .
JOURNAL OF MATERIALS SCIENCE, 1990, 25 (1A) :268-276
[2]   FORMATION AND GROWTH-MORPHOLOGY OF OXIDATION-INDUCED FERRITE LAYER IN FE-MN-AL-CR-C ALLOYS [J].
DUH, JG ;
WANG, CJ .
JOURNAL OF MATERIALS SCIENCE, 1990, 25 (04) :2063-2070
[3]   MICROSTRUCTURAL DEVELOPMENT IN THE OXIDATION-INDUCED PHASE-TRANSFORMATION OF FE-AL-CR-MN-C ALLOYS [J].
DUH, JG ;
LEE, JW ;
WANG, CJ .
JOURNAL OF MATERIALS SCIENCE, 1988, 23 (07) :2649-2660
[4]  
DUH JG, 1987, ALTERNATE ALLOYING E, P283
[5]   BEHAVIOR OF SELECTED COMMERCIAL ALLOYS DURING HIGH-TEMPERATURE OXYCHLORIDATION [J].
ELLIOTT, P ;
ANSARI, AA ;
PRESCOTT, R ;
ROTHMAN, MF .
CORROSION, 1988, 44 (08) :544-554
[6]   EFFECTS OF ALLOYING ELEMENTS ON NACL-INDUCED HOT CORROSION OF STAINLESS-STEELS [J].
HIRAMATSU, N ;
UEMATSU, Y ;
TANAKA, T ;
KINUGASA, M .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1989, 120 (1 -2 pt 1) :319-328
[7]   MICROSTRUCTURAL STUDY OF INFLUENCE OF NACL VAPOR ON OXIDATION OF A NI-CR-AL ALLOY AT 850-DEGREES-C [J].
HOSSAIN, MK ;
SAUNDERS, SRJ .
OXIDATION OF METALS, 1978, 12 (01) :1-22
[8]   THE OXIDATION OF BINARY IRON-MANGANESE ALLOYS [J].
JACKSON, PRS ;
WALLWORK, GR .
OXIDATION OF METALS, 1983, 20 (1-2) :1-17
[9]   HIGH-TEMPERATURE OXIDATION OF IRON-MANGANESE-ALUMINUM BASED ALLOYS [J].
JACKSON, PRS ;
WALLWORK, GR .
OXIDATION OF METALS, 1984, 21 (3-4) :135-170
[10]  
JAHN MT, 1987, ALTERNATE ALLOYING E, P179