摘要
The selective catalytic reduction (SCR) of NO by methane in the presence of excess oxygen has been studied on a series of Pd catalysts supported on sulfated zirconia (SZ). This support is not as sensitive to structural damage by steaming as the acidic zeolites, such as H-ZSM-5 and H-Mor. In previous studies, it was shown that this type of acidic zeolites are able to stabilize Pd2+ ions and promote high SCR activity and selectivity, which are typically not seen in Pd catalysts. In this contribution, it has been demonstrated that SZ is able to promote the NO reduction activity in a similar way to the acidic zeolites, by stabilizing Pd2+ ions that is selective for NO reduction. As in the case of acidic zeolites, the stabilization of Pd2+ ions can occur through a transfer of Pd species from particle to particle. One of the attractive features of Pd/SZ catalysts is that they are less sensitive to water and SO2 poisoning than Pd/H-ZSM-5 catalyst and exhibit higher reversibility after removal of water or SO2. (C)1999 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:419 / 429
页数:11
相关论文
共 22 条
[1]   The effect of zeolitic protons on NOx reduction over Pd/ZSM-5 catalysts [J].
Adelman, BJ ;
Sachtler, WMH .
APPLIED CATALYSIS B-ENVIRONMENTAL, 1997, 14 (1-2) :1-11
[2]   Redispersion of Pd on acidic supports and loss of methane combustion activity during the selective reduction of NO by CH4 [J].
Ali, A ;
Chin, YH ;
Resasco, DE .
CATALYSIS LETTERS, 1998, 56 (2-3) :111-117
[3]   State of Pd on H-ZSM-5 and other acidic supports during the selective reduction of NO by CH4 studied by EXAFS/XANES [J].
Ali, A ;
Alvarez, W ;
Loughran, CJ ;
Resasco, DE .
APPLIED CATALYSIS B-ENVIRONMENTAL, 1997, 14 (1-2) :13-22
[4]  
Alvarez WE, 1996, STUD SURF SCI CATAL, V101, P553
[5]   Investigations of the dispersion of Pd in H-ZSM-5 [J].
Aylor, AW ;
Lobree, LJ ;
Reimer, JA ;
Bell, AT .
JOURNAL OF CATALYSIS, 1997, 172 (02) :453-462
[6]  
BELL AT, 1998, P 1998 AICHE ANN M M
[7]  
CHIN Y, 1999, CATALYSIS, V14
[8]   Infrared study of nitrogen monoxide adsorption on palladium ion-exchanged ZSM-5 catalysts [J].
Descorme, C ;
Gelin, P ;
Primet, M ;
Lecuyer, C .
CATALYSIS LETTERS, 1996, 41 (3-4) :133-138
[9]  
DESCORME C, 1995, ZEOLITES REFINED TOO
[10]   CO AND NO INTERACTION WITH PD-AG AND PD-CR BIMETALLIC CATALYSTS .1. X-RAY-DIFFRACTION, INFRARED-SPECTROSCOPY, AND THERMOREACTION [J].
ELHAMDAOUI, A ;
BERGERET, G ;
MASSARDIER, J ;
PRIMET, M ;
RENOUPREZ, A .
JOURNAL OF CATALYSIS, 1994, 148 (01) :47-55