The effect of different siloxane chain-extenders on the thermal degradation and stability of segmented polyurethanes

被引:114
作者
Chuang, FS [1 ]
Tsen, WC [1 ]
Shu, YC [1 ]
机构
[1] Vanung Univ, Dept Text Sci, Tao Yuan 320, Taiwan
关键词
siloxane; polyurethane; thermal degradation; stability;
D O I
10.1016/j.polymdegradstab.2003.10.002
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The thermal degradation and stability of siloxane-containing segmented polyurethane and poly(urethane-urea) polymers (OH-SiPU and NH2-SiPU), both prepared from 4,4'-diphenylmethane diisocyanate (MDI), polytetramethylene ether glycol (PTMG) and silicon-containing chain-extenders, have been studied by thermogravimetric analysis (TGA) and Ozawa-Flynn kinetic analysis. The analyses identically revealed that OH-SiPU and NH2-SiPU polymers showed two stages of thermal degradation. The thermal stability and degradation depended on the kinds of hard and soft segment in the backbone of the polymers. The OH-SiPU polymers whose hard segment consists of siloxane-urethane displayed more thermal stability than the NH2-SiPU polymers, whose hard segment consist of siloxane-urea, in the initial degradation at the first stage of reaction (stage I). However, NH2-SiPU polymers were more thermally stable than OH-SiPU polymers and typical polyurethane as the weight loss went beyond about 5 wt.%. The length of the soft segment (PTMG molecular weight) affected the thermal stability of these polymers at various stage of degradation: polymers with a long soft segment had a high thermal stability in stage I, and those with a short soft segment had a higher thermal stability in the second stage of degradation (stage II). The Ozawa method was used to evaluate the activation the energies (Ea) of the whole process of degradation and the average activation energy (Ea,av) in each stage of degradation. The Ea and Ea,av values determined for the OH-SiPU and NH2-SiPU polymers according to the Ozawa method corresponds with the TG and DTG curve displaying the character of the degradation. (C) 2004 Elsevier Ltd. All rights reserved.
引用
收藏
页码:69 / 77
页数:9
相关论文
共 25 条
[1]   MECHANISM OF THERMAL-DEGRADATION OF POLYURETHANES INVESTIGATED BY DIRECT PYROLYSIS IN THE MASS-SPECTROMETER [J].
BALLISTRERI, A ;
FOTI, S ;
MARAVIGNA, P ;
MONTAUDO, G ;
SCAMPORRINO, E .
JOURNAL OF POLYMER SCIENCE PART A-POLYMER CHEMISTRY, 1980, 18 (06) :1923-1931
[2]   SYNTHESIS OF NEW SILOXANE URETHANE BLOCK-COPOLYMERS AND THEIR PROPERTIES [J].
BENRASHID, R ;
NELSON, GL .
JOURNAL OF POLYMER SCIENCE PART A-POLYMER CHEMISTRY, 1994, 32 (10) :1847-1865
[3]   The effect of silicon and phosphorus on the degradation of poly(methyl methacrylate) [J].
Chang, TC ;
Chen, YC ;
Ho, SY ;
Chiu, YS .
POLYMER, 1996, 37 (14) :2963-2968
[4]   Characterization and degradation of some silicon-containing polyimides [J].
Chang, TC ;
Wu, KH .
POLYMER DEGRADATION AND STABILITY, 1998, 60 (01) :161-168
[5]  
FEDOTOVA OY, 1969, POLYM SCI USSR, V11, P3123
[6]   THERMAL-STABILITY OF SEGMENTED POLYURETHANES [J].
FERGUSON, J ;
PETROVIC, Z .
EUROPEAN POLYMER JOURNAL, 1976, 12 (03) :177-181
[7]  
GASSIE N, 1978, J POLYM SCI POL CHEM, V16, P1563
[8]   LIMITING OXYGEN INDEXES OF SILICONE BLOCK POLYMERS [J].
KAMBOUR, RP ;
KLOPFER, HJ ;
SMITH, SA .
JOURNAL OF APPLIED POLYMER SCIENCE, 1981, 26 (03) :847-859
[9]  
KOTOMKIN VY, 1981, PLAST MASSY, P27